The role of hydride, martensite and atomic hydrogen in hydrogen-induced delayed fracture of TiNi alloy
Authors:
- J.Y. HeJHJ.Y. He
- K.W. GaoKGK.W. Gao
- Y.J. SuYSY.J. Su
- L.J. QiaoLQL.J. Qiao
- W.Y. ChuWCW.Y. Chu
- 1 January 2004
- journal article
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 364 (1-2) , 333-338
Abstract
No abstract availableKeywords
This publication has 14 references indexed in Scilit:
- Susceptibility to delayed fracture of Ni–Ti superelastic alloyMaterials Science and Engineering: A, 2003
- Hydrogen embrittlement of nickel-titanium alloy in biological environmentMetallurgical and Materials Transactions A, 2002
- Martensitic transition in a Ni40Ti50Cu10 alloy containing hydrogen: calorimetric (DSC) and mechanical spectroscopy experimentsScripta Materialia, 2001
- Fracture Analysis of Hydrogen-Charged Nickel-Titanium Superelastic AlloyMATERIALS TRANSACTIONS, 2001
- Prediction of threshold stress intensity factor for hydrogen induced intergranular cracking of tubular steelMaterials Science and Engineering: A, 2000
- An overview of nitinol medical applicationsMaterials Science and Engineering: A, 1999
- Hydrogen Accumulation and Hydrogen-Induced Cracking of API C90 Tubular SteelCorrosion, 1997
- Structural study of the hydrides NiTiHx (X = 1.0 and 1.4)Journal of Alloys and Compounds, 1993
- Effect of Hydrogen on the Shape Memory Effect and Transformation Behavior of Ti-Ni AlloyJournal of the Japan Institute of Metals and Materials, 1990
- Pseudoelasticity and shape memory effects in alloysInternational Materials Reviews, 1986