Abstract
Ce3+Ce3+ luminescence is studied for the first time in BaMgSiO4BaMgSiO4 . Intense and broad blue emission is observed with maximum at 430nm430nm when excited with 356nm356nm . Studies on Ba1−2yCeyLiyMgSiO4Ba1−2yCeyLiyMgSiO4 (y=0.0025−0.125)(y=0.0025−0.125) show that the emission intensity is maximum for y=0.1y=0.1 and a decrease in emission intensity is observed for higher yy values. The concentration of Eu2+Eu2+ and Ce3+Ce3+ are varied in BaMgSiO4:0.1Ce3+BaMgSiO4:0.1Ce3+ , Eu2+Eu2+ , and BaMgSiO4:0.01Eu2+BaMgSiO4:0.01Eu2+ , Ce3+Ce3+ systems, respectively, in order to find the critical concentration of Eu2+Eu2+ and Ce3+Ce3+ to achieve high emission intensity of Eu2+Eu2+ . Ba0.75Eu0.05Ce0.1Li0.1MgSiO4Ba0.75Eu0.05Ce0.1Li0.1MgSiO4 and Ba0.97Eu0.01Ce0.01Li0.01MgSiO4Ba0.97Eu0.01Ce0.01Li0.01MgSiO4 compositions show maximum Eu2+Eu2+ emission, and the emission intensity is found to be comparable with that of commercial ZnS:Cu,AlZnS:Cu,Al (green phosphor, SONY) under near-UV excitation (400nm)(400nm) . Commission Internationale de I’Eclairage (CIE) chromaticity coordinates indicate that the Eu2+Eu2+ and Ce3+Ce3+ substituted compositions are potential green phosphors for solid-state lighting, light-emitting diode technology.

This publication has 11 references indexed in Scilit: