A fine, uniform A1 2 O 3 ‐SiO 2 powder was prepared by heterocoagulation of narrow Al 2 O 3 and SiO 2 powders. This composite powder was dispersed, compacted, and fired in air at 900° to 1580°C for 1 to 13 h. Full density was achieved at 1550°C with the formation of a mullite phase. Relative densities of 83% and 98% (0.3 μm grain size) were measured for samples sintered at 1200°C for 13 h and at 1400°C for 1 h, respectively.