Abstract
Low-temperature sintering of Cu particles has considerable potential for advanced power electronic packaging, but surface oxidation and insufficient atomic diffusion at low temperatures limit the performance of sintering joints. In this paper, an ultrasonic-assisted sintering process was proposed and optimized, and the effect of the ultrasonic process and sintering temperature on the microstructure and properties of the Cu-Cu sintered joints was investigated. Without ultrasonic assistance, the average shear strength increased from 6.12 MPa to 46.73 MPa as the sintering temperature increased from 200°C to 240 °C, which was primarily attributable to the temperature promoting atomic diffusion. The joint performance showed a trend of increasing first and then decreasing with the increase of ultrasonic power and duration under the ultrasonic-assisted process at 200°C. The best performance was obtained at 600 W for 4 s, giving a shear strength of 43.35 MPa, approximately 7.1 times higher than that without ultrasonic assistance at 200°C, approaching the shear strength of the sintered joint without ultrasonic-assisted sintering at 240℃. However, excessively high ultrasonic power and duration could damage the sintered layer, cause micro-cracks, and reduce performance. Microstructural analysis indicates that moderate ultrasonic treatment could promote surface-oxide disruption, particle rearrangement, and plastic deformation, thereby facilitating atomic diffusion and sintering-neck growth at low temperatures, and transforming the fracture path from interface separation to internal cohesive fracture. This study proposed an ultrasonic-assisted process for copper particle low-temperature sintering and elucidated its strengthening mechanism, providing a basis for Cu-Cu bonding in low thermal budget power devices.

This publication has 24 references indexed in Scilit: