This study assessed the shear bond strength (SBS) and failure modes of lithium disilicate ceramic veneering material to different high-performance polymers. Thirty-six square specimens measuring 7 × 7 × 2 ± 0.05 mm were prepared from pure polyetheretherketone (PEEK), Bio-high performance PEEK (BioHPP) and Trilor discs. Polymer specimens were air-borne abraded utilizing aluminum oxide particles, cleaned, and a bonding agent was applied (visio. link). The veneering LDC material (3 × 2 mm) was milled, hydrofluoric acid etched (9.5%) and primed (Clearfil ceramic). The LDC was bonded to the polymer specimens using dual-cured resin cement (Panavia V5) and light polymerized. The bonded specimens were subjected to 5000 cycles of physiological aging by thermocycling, and the SBS test was performed in a universal testing machine at 0.5 mm/min cross-head speed. The debonded specimens were analyzed to determine the primary bond failure sites (adhesive, mixed or cohesive). Data analysis was performed using one-way ANOVA and a post hoc Tukey test (α ≤ 0.05). The BioHPP material demonstrated the highest SBS values (23.94 ± 1.43 MPa), and the Trilor group recorded the lowest SBS values (17.09 ± 1.07 MPa). The PEEK group showed a mean SBS of 21.21 ± 1.51 MPa. The SBS comparison showed significant variations across all material groups (p < 0.001). Regarding failure modes, adhesive failure was observed in 40% of BioHPP and PEEK specimens and 90% of Trilor specimens. The cohesive failure occurred in 50% of PEEK and 30% of BioHPP specimens, while the Trilor specimens showed no cohesive failure. Mixed failures were reported in 30% of BioHPP and 10% of PEEK and Trilor specimens. The BioHPP material demonstrated high SBS followed by PEEK and Trilor. The SBS between the tested materials was statistically significant. However, the SBS of the tested implant framework materials was above the limit stipulated by the ISO 10477 standard (5 MPa) and the clinically acceptable range of 10–12 MPa.Keywords
This publication has 53 references indexed in Scilit:
- Polyaryletherketones: Properties and applications in modern medicineBiomedical Technology, 2024
- Recent advances of additive manufacturing in implant fabrication – A reviewApplied Surface Science Advances, 2023
- Effect of veneering material type and thickness ratio on flexural strength of bi-layered PEEK restorations before and after thermal cyclingClinical Oral Investigations, 2023
- Long-term chipping and failure rates of implant-supported and combined tooth–implant-supported metal-ceramic and ceramic fixed dental prostheses: A cohort studyThe Journal of Prosthetic Dentistry, 2021
- Responses of pre-crystallized and crystallized zirconia-containing lithium silicate glass ceramics to diamond machiningCeramics International, 2020
- Comparative evaluation of BioHPP and titanium as a framework veneered with composite resin for implant-supported fixed dental prosthesesThe Journal of Prosthetic Dentistry, 2019
- Effect of repeated ceramic firings on the marginal and internal adaptation of metal ceramic restorations fabricated with different CAD-CAM technologiesThe Journal of Prosthetic Dentistry, 2017
- Pressure behavior of different PEEK materials for dental implantsJournal of the Mechanical Behavior of Biomedical Materials, 2016
- Thermal cycling for restorative materials: Does a standardized protocol exist in laboratory testing? A literature reviewJournal of the Mechanical Behavior of Biomedical Materials, 2014
- Elastic properties and apparent density of human edentulous maxilla and mandibleInternational Journal of Oral and Maxillofacial Surgery, 2009