Abstract
Achieving tritium self-sufficiency remains a key challenge for future fusion reactors, creating a strong need for breeder materials with efficient tritium release. In this study, neutron-irradiated Li 2 Pb x Ti 1− x O 3 ( x = 0, 0.05, and 0.1) ceramic pebbles were investigated by tritium thermal desorption spectroscopy (T-TDS) and electron spin resonance (ESR). Tritium release was examined at different heating rates and under isothermal conditions, and the corresponding kinetic parameters were determined. All samples exhibited a single tritium desorption peak that shifted to higher temperatures with increasing heating rate, confirming a thermally activated release process. Pb introduction broadened the desorption peak and lowered the apparent activation energy for tritium release. Under isothermal heating, the tritium diffusion activation energy ( E d ) and pre-exponential factor ( D 0 ) increased simultaneously, following the compensation effect and suggesting multiple migration pathways. ESR isochronal and isothermal annealing showed that irradiation-defect annihilation occurs in two stages: a fast stage associated with electron migration and a slower stage governed by oxygen diffusion. The defect-annihilation range overlaps strongly with the main tritium-release range, indicating that tritium release is jointly controlled by diffusion and defect evolution. Increasing Pb content modifies irradiation-defect annealing behavior and influences tritium-release kinetics.Keywords
Funding Information
- The National MCF Energy R&D Program (2022YFE03210200)
- The National MCF Energy R&D Program (2024YFE03250100)
- The National Natural Science Foundation of China (12475303)
- The National Natural Science Foundation of China (12575288)
- The National Natural Science Foundation of China (12205070)
- The National Natural Science Foundation of China (12205071)
- The National Natural Science Foundation of China (12305292)
- the Fundamental Research Funds for the Central Universities (PA2025GDGP0025)
- the Fundamental Research Funds for the Central Universities (PA2024GDGP0042)
This publication has 45 references indexed in Scilit:
- Hyper-stoichiometric lithium titanate for tritium breeding applicationCeramics International, 2025
- Tritium release performance of biphasic Li2TiO3–Li4SiO4 ceramic pebbles fabricated by centrifugal granulation methodCeramics International, 2024
- Fabrication, sintering behavior, and strength of tritium breeding ceramic pebbles with Pb additionCeramics International, 2024
- Tritium and deuterium release behavior of Li2TiO3-0.5Li4SiO4–Pb ceramicCeramics International, 2023
- Measurement of neutron flux parameters for implementation of k0-INAA at Kyoto University Research ReactorJournal of Radioanalytical and Nuclear Chemistry, 2022
- Solution combustion synthesis of lithium orthosilicate as the tritium breeder: Effects of microwave power and fuel-to-oxidizer ratio on phase, microstructure and sinteringCeramics International, 2021
- Kinetics and mechanism of thermal degradation of pentose- and hexose-based carbohydrate polymersCarbohydrate Polymers, 2012
- Hot atom chemical behavior of tritium in neutron-irradiated Li2TiO3 and Li2ZrO3Journal of Radioanalytical and Nuclear Chemistry, 2007
- Chemical states of tritium and interaction with radiation damages in Li2O crystalsJournal of Nuclear Materials, 1986
- Experimental study of the Pb and Bi breeding zones effect on the neutron parameters of a molten-salt blanket in a fusion reactorNuclear Instruments and Methods, 1980