Finite element analysis of SCALPEL wafer heating
Authors:
- Stuart T. StantonSSStuart T. Stanton
- J. Alexander LiddleJLJ. Alexander Liddle
- A. EhrmannAEA. Ehrmann
- T. StruckTST. Struck
- A. ChalupkaACA. Chalupka
- E. HaugenederEHE. Haugeneder
- H. LöschnerHLH. Löschner
- J. ButschkeJBJ. Butschke
- 1 November 1999
- journal article
- Published by American Vacuum Society in Journal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena
- Vol. 17 (6) , 2883-2887
Abstract
A high-throughput scattering with angular limitation projection electron beam lithography (SCALPEL) tool will typically deliver up to to an area of 250 μm×250 μm over a time of 200 μs, corresponding to a power input of 0.75 W. This heat deposition occurs in the upper 60 μm of a wafer creating local thermal strain at the time of image formation, and depends on mask and tool conditions and specific boundary conditions. Initial modeling results indicate expansion-induced peak pattern placement errors of ∼1 nm on a local scale (i.e., a 3 mm effective field size), several nanometers in a chip area, and a few microns overall. Since the use of a mainly predictive correction algorithm is anticipated, it is vital to conduct a rigorous investigation of the heat transfer and strain formation. Results are presented of such an analysis, illustrating the heating response for the fundamental building blocks of the SCALPEL writing strategy.
Keywords
This publication has 6 references indexed in Scilit:
- Electron optical analysis of SCALPEL writing strategy1999
- Writing strategy for a high-throughput SCALPEL system1999
- Initial wafer heating analysis for a SCALPEL lithography systemMicroelectronic Engineering, 1999
- Simulation of resist heating in electron-beam lithography1997
- Resist Heating in Cell Projection Electron Beam Direct WritingJapanese Journal of Applied Physics, 1997
- New approach to projection-electron lithography with demonstrated 0.1 μm linewidthApplied Physics Letters, 1990