Abstract
This paper describes work carried out on flame‐retarded polypropylene comparing results on selected small‐scale laboratory fire tests with those obtained on a larger‐scale test designed to simulate the typical real life hazard situation. In the latter test a number of important parameters such as heat build‐up, Hame spread, smoke development and gas evolution were assessed. The results indicate that there is need to use both types of tests to gain a fuller understanding prior to using new materials. An assessment based on small‐scale tests alone could be misleading and allow the use of potentially hazardous material in the particular application involved.