Abstract
Composites with varied proportions of β-Ca3(PO4)2 and ZnO were obtained through an in situ aqueous precipitation method under slightly basic (pH ≈ 8) conditions. The formation of β-Ca3(PO4)2 phase starts at an early heat-treatment stage (∼800 °C) and incorporates Zn2+ ions at both Ca2+(4) and Ca2+(5) sites of the lattice up to its occupancy saturation limit. The incorporation of Zn2+ in the β-Ca3(PO4)2 lattice enhances its thermal stability delaying the allotropic β-Ca3(PO4)2→α-Ca3(PO4)2 phase transformation. The excess zinc beyond the occupancy saturation limit precipitates as Zn(OH)2 and undergoes dehydroxylation to form ZnO at elevated temperatures. The presence of ZnO in the β-Ca3(PO4)2 matrix yields denser microstructures and thus improves the mechanical features of sintered composites up to an optimal ZnO concentration beyond which it tends to exert an opposite effect.
Funding Information
  • Council of Scientific and Industrial Research (22(612)/12/EMRI)
  • European Regional Development Fund
  • Fundação para a Ciência e a Tecnologia (UID/CTM/50011/2013)

This publication has 55 references indexed in Scilit: