Effect of the sintering technique on the ferroelectric and d33 piezoelectric coefficients of Bi0.5(Na0.84K0.16)0.5TiO3 ceramic
Open Access
- 21 May 2019
- journal article
- research article
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 8 (2) , 278-288
Abstract
In the search of lead-free piezoelectric materials, ceramic processing techniques offer potential tools to increase the piezoelectric and ferroelectric properties in addition to new chemical compositions. Powders of pure BNKT16 (Bi0.5(Na0.84K0.16)0.5TiO3) phase were synthesized by sol-gel method with a low crystallization temperature (750 °C). Ceramic samples were sintered by pressureless sintering (PLS), sinter-forging (SF), and spark plasma sintering (SPS) techniques. Structural, morphological, and chemical characterizations were performed by XRD, Raman, EDS, and SEM. Sintered samples by PLS and SF exhibit rod-like grains associated to bismuth volatility. The highest remanent polarization (11.05 µC/cm2), coercive field (26.2 kV/mm), and piezoelectric coefficient (165 pC/N) were obtained for SF sample. The piezoresponse force microscopy (PFM) analysis shows that the crystallites at the nanoscale exhibit piezoelectric phenomenon and the highest piezoelectric response is reported for PLS sample. The presence of the rhombohedral phase, the increase in grain and crystallite size, and the oriented rod-like inclusions favoring the crystallographic texture are facts that enhance the piezoelectric coefficient for BNKT16 piezoceramics.Keywords
This publication has 36 references indexed in Scilit:
- Dielectric properties of Bismuth Titanate densified by Spark Plasma Sintering and Pressureless SinteringJournal of Alloys and Compounds, 2012
- Comparative Study between Conventional and Microwave Sintered Lead-Free BNKT CeramicsFerroelectrics, 2009
- Perspective on the Development of Lead‐free PiezoceramicsJournal of the American Ceramic Society, 2009
- Study of the morphotropic phase boundary in the lead-free Na1/2Bi1/2TiO3-BaTiO3 system by Raman spectroscopyJournal of the Ceramic Society of Japan, 2009
- Simulation of the Stress‐Assisted Densification Behavior of a Powder Compact: Effect of Constitutive LawsJournal of the American Ceramic Society, 2008
- Nanoscale ferroelectrics: processing, characterization and future trendsReports on Progress in Physics, 2006
- Phase transition, ferroelectric behaviors and domain structures of (Na1/2Bi1/2)1−xTiPbxO3 thin filmsActa Materialia, 2006
- Spark Plasma Sintering of Bismuth Titanate CeramicsJournal of the American Ceramic Society, 2005
- Preparation of Textured Bismuth Titanate Ceramics Using Spark Plasma SinteringJournal of the American Ceramic Society, 2004
- A structural study of the (Na
1−
x
K
x
) 0.5 Bi 0.5 TiO 3 perovskite series as a function of substitution ( x ) and temperaturePowder Diffraction, 2002