Fabrication of an all-oxide thermoelectric power generator

Authors:

Abstract
An oxide thermoelectric device was fabricated using Gd-doped Ca3Co4O9 p -type legs and La-doped CaMnO3 n -type legs on a fin. The power factors of p legs and n legs were 4.8×10−4 Wm−1 K−2 and 2.2×10−4 Wm−1 K−2 at 700 °C in air, respectively. With eight p–n couples the device generated an output power of 63.5 mW under the thermal condition of hot side temperature Th=773 °C and a temperature difference ΔT=390 °C. This device proved to be operable for more than two weeks in air showing high durability.