Effect of Nickel-Containing Catalyst on the Tar Coking Process
Authors:
- 1 April 2021
- journal article
- research article
- Published by Pleiades Publishing Ltd in Catalysis in Industry
- Vol. 13 (2) , 143-149
Abstract
Coking has been studied with and without the 7% Ni/CNT catalyst. It has been shown that tar coking results in the formation of gaseous and liquid products and petroleum coke at a temperature of 350°C without the catalyst. Thermolysis products are formed due to the elimination of side hydrocarbon chains from the initial polyaromatic hydrocarbons. Gaseous products consist of C1–C6 hydrocarbons and sulfur-containing gases H2S and COS. The fractional composition of liquid thermolysis products is studied. It has been found that 50% of the liquid products are gasoline and diesel fractions. The 7% Ni/CNT catalyst is prepared via impregnation. The effect of the 7% Ni/CNT catalyst on the tar coking process in the 300–550°C range of temperatures is studied. The addition of the 7% Ni/CNT catalyst to tar increases the yield and lowers the content of sulfur in petroleum coke due to the conversion of some into hydrogen sulfide and COS, which are removed with the gas phase. Electron microscope study shows that the petroleum coke resulting from the catalytic coking of tar proves to be reinforced with carbon nanotubes.Keywords
This publication has 8 references indexed in Scilit:
- Hexadecane Conversion on an Alumina–Nickel CatalystKinetics and Catalysis, 2019
- Effect of Carbon Nanotube Admixture on Anthracene CokingPetroleum Chemistry, 2019
- Effect of “Cobalt–Carbon Nanotubes” Catalysts on Anthracene CokingDoklady Physical Chemistry, 2019
- Formation of Carbon from High-Molecular Hydrocarbons on Iron Subgroup Metals on the Sibunite Carbon SupportCatalysis in Industry, 2018
- Catalyst and technology for production of carbon nanotubesKinetics and Catalysis, 2010
- Delayed Coker Coke Morphology Fundamentals: Mechanistic Implications Based on XPS Analysis of the Composition of Vanadium- and Nickel-Containing Additives during Coke FormationEnergy & Fuels, 2007
- The formation of carbon filaments upon decomposition of hydrocarbons catalysed by iron subgroup metals and their alloysRussian Chemical Reviews, 2000
- The structure of graphitic carbonsActa Crystallographica, 1951