Superconducting Properties and Anisotropic Electrical Resistivities of Pure and Cadmium-Doped Tin

Authors:

Abstract
Approximately 60 cylindrically shaped single crystals of pure and cadmium-doped (ρ(T) for pure tin was determined. ρII(T)ρ⊥(T) is found to be 1.53±0.01 at 373°K, 1.555±0.009 at 273°K, and 1.684±0.010 at 77°K. ρ⊥(T) is 13.25±0.05, 9.05±0.03, and 1.772±0.006 μΩ-cm at 373, 272, and 77°K respectively. The anisotropy of the residual resistivity ρ0 for cadmium impurity was determined at 4.2°K by two different experimental methods in different regions of impurity concentration x. ρ0IIρ0⊥ is found to be 1.6±0.1 in both regions. The residual resistivity for any specific crystal orientation is found to vary linearly with x (ρ0⊥x=1.39 μΩ cm/at.%). Deviations from Matthiessen's rule are found to vary linearly [ρ(T)impure−ρ(T)pure=0.16ρ0⊥] with impurity concentration and appear to be temperature-independent for 77°K≤T≤373°K. The general features of the data relating the change in superconducting transition temperature (Tc) with doping are in good agreement with the data of Lynton, Serin, and Zucker. However, there is evidence for anomalous Tc behavior in the region of composition (x≈0.3%) at which a lattice-spacing anomaly was reported by Lee and Raynor. The development of vacant sites as reported by Lee and Raynor in this region is not observed in plots of ρ0⊥ versus x, however. The theory of Markowitz and Kadanoff is applied to the data relating Tc to impurity concentration. Reasonable agreement between the theory and experiment is found. The mean-squared relative anisotropy of the superconducting energy gap parameter 〈a2〉, is found from this analysis to be 0.023. A recent theoretical treatment due to Clem which describes the change in the critical-field parameters with doping is compared to our experimental results. The so-called "similarity conditions" are found not to be satisfied. The shape of the reduced critical-field curve is found to be a function of impurity concentration. The value of 〈a2〉 obtained from our data employing Clem's equations is 0.022, in good agreement with the value obtained from the Tc data alone. The data describing the reduced critical-field curve of pure tin is in good agreement with the results od Shaw et al. The change in shape of the reduced critical-field curve can be understood both qualitatively and quantitatively in terms of the reduction of the effects of 〈a2〉 with doping as given by Clem's theoretical treatment.

This publication has 27 references indexed in Scilit: