Abstract
SUMMARY: Objective: This in vitro study evaluated the shear bond strength of composite resin to deep dentin using a total etch adhesive after treatment with two collagen cross-linking agents at varying time intervals. Materials and Methods: Thirty freshly extracted human maxillary central incisors were sectioned longitudinally into equal mesial and distal halves (n=60). The proximal deep dentin was exposed, maintaining a remaining dentin thickness (RDT) of approximately 1 mm. The specimens were randomly divided into three groups based on the surface treatment of dentin prior to bonding as follows: group I (n=12, control): no prior dentin surface treatment; group II (n=24): dentin surface pretreated with 10% sodium ascorbate; and group III (n=24): dentin surface pretreated with 6.5% proanthocyanidin. Groups II and III were further subdivided into two subgroups of 12 specimens each, based on the pretreatment time of five minutes (subgroup A) and 10 minutes (subgroup B). Shear bond strength of the specimens was tested with a universal testing machine, and the data were statistically analyzed. Results: Significantly higher shear bond strength to deep dentin was observed in teeth treated with 10% sodium ascorbate (group II) and 6.5% proanthocyanidin (group III) compared to the control group (group I). Among the collagen cross-linkers used, specimens treated with proanthocyanidin showed significantly higher shear bond strength values than those treated with sodium ascorbate. No significant difference was observed between the five-minute and 10-minute pretreatment times in groups II and III. Conclusion: It can be concluded that dentin surface pretreatment with both 10% sodium ascorbate and 6.5% proanthocyanidin resulted in significant improvement in bond strength of resin composite to deep dentin.Keywords
This publication has 24 references indexed in Scilit:
- Variations in collagen fibrils network structure and surface dehydration of acid demineralized intertubular dentin: Effect of dentin depth and air-exposure timeDental Materials, 2010
- A three-year clinical evaluation of two-bottle versus one-bottle dentin adhesivesThe Journal of the American Dental Association, 2005
- Single-step adhesives are permeable membranesJournal of Dentistry, 2002
- Clinical evaluation of two one-bottle dentin adhesives at three yearsThe Journal of the American Dental Association, 2001
- Relation between water content in acetone/alcohol-based primer and interfacial ultrastructureJournal of Dentistry, 1998
- The dentin substrate: structure and properties related to bondingJournal of Dentistry, 1997
- Dentine permeability and dentine adhesionJournal of Dentistry, 1997
- The influence of age and depth of dentin on bondingDental Materials, 1994
- Correlation among dentin depth, permeability, and bond strength of adhesive resinsDental Materials, 1990
- The promotion of adhesion by the infiltration of monomers into tooth substratesJournal of Biomedical Materials Research, 1982