Effects of Hydrofluoric Acid Concentrations, Commercial Brands, and Adhesive Application on the Bond Strength of a Resin Luting Agent to Lithium Disilicate Glass Ceramic
Authors:
- 1 November 2023
- journal article
- research article
- Published by Operative Dentistry in Operative Dentistry
- Vol. 48 (6) , 700-710
Abstract
SUMMARY: Objectives: To evaluate the surface topography/roughness and bond strength of a resin luting agent to a lithium disilicate glass ceramic after etching with different concentrations of hydrofluoric acid (HF) and commercial brands. Methods: For bond strength evaluation, 260 lithium disilicate glass ceramic (EMX) discs were randomly distributed into 13 groups based on concentrations of HF and commercial brands (n=20): 5% and 10%, Lysanda (LY5 and LY10); 5% and 10%, Maquira (MA5 and MA10); 5% and 10%, FGM (FG5 and FG10); 4.8%, Ivoclar Vivadent (IV5); 5% and 10%, PHS do Brasil (PH5 and PH10); 5% and 10%, BM4 (BM5 and BM10); 9%, Ultradent Inc (UL10); and Dentsply (DE10). A further random distribution (n=10) was made based on the application (+) or absence (−) of an adhesive layer. Resin luting agent cylinders (1 mm in diameter) were added on EMX surfaces, light-cured, and stored for 24 hours in deionized water at 37°C. On a universal testing machine (DL 500, EMIC), specimens were submitted to a microshear bond strength test at a crosshead speed of 1 mm/min until failure. A representative etched EMX disc from each group underwent surface topography analysis using field-emission scanning electron microscopy (n=1), and five (n=5) etched EMX discs from each group were tested for surface roughness. Data were statistically analyzed using analysis of variance and Tukey test (α=0.05). Results: A less conditioned and smoother surface was observed for 5% HF compared to 10%. Additionally, commercial brands of HF were shown to affect bond strength. When the adhesive layer was not used (−), a 10% concentration promoted higher bond strengths to EMX. However, when adhesive was applied (+), the concentrations of HF and commercial brands had no effect on bond strength results. Conclusions: A 10% concentration of HF results in higher bond strength than a 5% concentration. If an adhesive layer is applied, neither this distinction nor the influence of commercial brands is observed.Keywords
This publication has 31 references indexed in Scilit:
- Lithium disilicate posterior overlays: clinical and biomechanical featuresClinical Oral Investigations, 2019
- Properties of hot-pressed lithium silicate glass-ceramicsDental Materials, 2019
- Ten-year survival and complication rates of lithium-disilicate (Empress 2) tooth-supported crowns, implant-supported crowns, and fixed dental prosthesesJournal of Dentistry, 2017
- Heat treatment-improved bond strength of resin cement to lithium disilicate dental glass-ceramicCeramics International, 2016
- Effect of etching time and resin bond on the flexural strength of IPS e.max Press glass ceramicDental Materials, 2014
- Aspects of bonding between resin luting cements and glass ceramic materialsDental Materials, 2014
- Possible hazardous effects of hydrofluoric acid and recommendations for treatment approach: a reviewClinical Oral Investigations, 2011
- State of the art of self-etch adhesivesDental Materials, 2011
- State of the art etch-and-rinse adhesivesDental Materials, 2011
- A comparison of the microstructure and properties of the IPS Empress 2 and the IPS Empress glass-ceramicsJournal of Biomedical Materials Research, 2000