Analysis of Failed Commercially Pure Titanium Dental Implants: A Scanning Electron Microscopy and Energy‐Dispersive Spectrometer X‐Ray Study
Authors:
- Jamil Awad ShibliJamil Awad Shibli
- Elcio MarcantonioEMElcio Marcantonio
- Susana D'AVilaSDSusana D'AVila
- Antonio Carlos GuastaldiAGAntonio Carlos Guastaldi
- 1 July 2005
- journal article
- Published by Wiley in Journal of Periodontology
- Vol. 76 (7) , 1092-1099
Abstract
Background: The failure of osseointegration in oral rehabilitation has gained importance in current literature and in clinical practice. The integration of titanium dental implants in alveolar bone has been partly ascribed to the biocompatibility of the implant surface oxide layer. The aim of this investigation was to analyze the surface topography and composition of failed titanium dental implants in order to determine possible causes of failure.Methods: Twenty‐one commercially pure titanium (cpTi) implants were retrieved from 16 patients (mean age of 50.33 ± 11.81 years). Fourteen implants were retrieved before loading (early failures), six after loading (late failures), and one because of mandibular canal damage. The failure criterion was lack of osseointegration characterized as dental implant mobility. Two unused implants were used as a control group. All implant surfaces were examined by scanning electron microscopy (SEM) and energy‐dispersive spectrometer x‐ray (EDS) to element analysis. Evaluations were performed on several locations of the same implant.Results: SEM showed that the surface of all retrieved implants consisted of different degrees of organic residues, appearing mainly as dark stains. The surface topography presented as grooves and ridges along the machined surface similar to control group. Overall, foreign elements such as carbon, oxygen, sodium, calcium, silicon, and aluminum were detected in failed implants. The implants from control group presented no macroscopic contamination and clear signs of titanium.Conclusion: These preliminary results do not suggest any material‐related cause for implant failures, although different element composition was assessed between failed implants and control implants. J Periodontol 2005;76:1092‐1099.Keywords
This publication has 20 references indexed in Scilit:
- The Effect of CO2 Laser Irradiation on Failed Implant SurfacesImplant Dentistry, 2004
- Treatment of Ligature‐Induced Peri‐Implantitis by Lethal Photosensitization and Guided Bone Regeneration: A Preliminary Histologic Study in DogsJournal of Periodontology, 2003
- Effect of Air-Powder System on Titanium Surface on Fibroblast Adhesion and MorphologyImplant Dentistry, 2003
- Quantitative and qualitative investigations of surface enlarged titanium and titanium alloy implantsClinical Oral Implants Research, 1998
- Surface spectroscopic characterization of titanium implant materialsJournal of Electron Spectroscopy and Related Phenomena, 1996
- Microbial aspects of implant dentistryPeriodontology 2000, 1994
- Surface spectroscopic characterization of titanium implant materialsApplied Surface Science, 1990
- Surface properties determine bioadhesive outcomes: Methods and resultsJournal of Biomedical Materials Research, 1984
- Osseointegrated Titanium Implants:Requirements for Ensuring a Long-Lasting, Direct Bone-to-Implant Anchorage in ManActa Orthopaedica, 1981
- Changes in nonosseous tissue adjacent to titanium implantsJournal of Biomedical Materials Research, 1973