Abstract
Na-substituted 122-type iron-based superconductors were synthesized and fabricated into superconducting tapes and wires. Good $J_c$ performance of Ag-sheathed $\rm Sr_{0.45}Na_{0.55}Fe_{2}As_{2}$ pressed tapes was demonstrated, and it was further improved by using AgSn as a sheath material. The improved $J_c$ characteristics is due to the reduction of the optimum sintering temperature by ∼100°C, which suppressed the reaction between the sheath and core. However, fabrication of good $\rm Sr_{0.45}Na_{0.55}Fe_{2}As_{2}$ round wire using the hot isostatic press method failed due possibly to the segregation of Na in the core. To avoid the segregation of Na, we fabricated round wires employing (Ba,Na) $\rm Fe_{2}As_{2}$ rather than underdoped (Sr,Na) $\rm Fe_{2}As_{2}$ . $J_c$ in $\rm Ba_{0.6}Na_{0.4}Fe_{2}As_{2}$ round wire processed 700°C under the pressure of 175 MPa reached $\rm 1.5\times 10^{5} A/cm^2 and 2.0\times 10^4 A/cm^2$ at self-field and 100 kOe, respectively. These values are more than half the value of record-high $J_c$ of (Ba,K) $\rm Fe_{2}As_{2}$ round wires, demonstrating the excellent performance of (Ba,Na) $\rm Fe_{2}As_2$ wires.
Funding Information
  • JSPS KAKENHI (17H01141)

This publication has 24 references indexed in Scilit: