Effect of magnetocrystalline anisotropy on the magnetic properties of Fe-rich R–Fe–B nanocomposite magnets
Authors:
- 11 October 1999
- journal article
- Published by AIP Publishing in Applied Physics Letters
- Vol. 75 (15) , 2298-2300
Abstract
Nanocomposite ribbons consisting of hard-magnetic R2Fe14B (R=rare-earth) and soft-magnetic Fe3B phases were produced by melt spinning and subsequent heat treatment. Alloys of composition Nd4−xSmxFe77.5B18.5, with x=0.0, 0.1, 0.2, 0.3, 0.4, and 0.5 all showing strong remanence enhancement, were selected to investigate the effect of the magnetocrystalline anisotropy of the R2Fe14B-type phase on the exchange coupling with the soft-magnetic phase in the nanocomposite magnets. An enhancement of exchange coupling due to anisotropy reduction was found, as expected on the basis of the model of Kneller and Hawig. A maximum of the energy product (BH)max was achieved for x=0.2 after annealing at 700 °C. The thermomagnetic behavior also changes upon substitution of Sm for Nd.Keywords
This publication has 7 references indexed in Scilit:
- Coercivity in lean rare earth NdFeB and PrFeB nanocomposite hard magnetic materialsJournal of Alloys and Compounds, 1998
- Two- and three-dimensional calculation of remanence enhancement of rare-earth based composite magnets (invited)Journal of Applied Physics, 1994
- New nanocrystalline high-remanence Nd-Fe-B alloys by rapid solidificationJournal of Magnetism and Magnetic Materials, 1993
- The exchange-spring magnet: a new material principle for permanent magnetsIEEE Transactions on Magnetics, 1991
- Magnetic properties of rapidly quenched NdFeB alloys with lower Nd concentrationSolid State Communications, 1990
- Analysis of the magnetic hardening mechanism in RE-FeB permanent magnetsJournal of Magnetism and Magnetic Materials, 1988
- A Numerical Fourier-analysis Method for the Correction of Widths and Shapes of Lines on X-ray Powder PhotographsProceedings of the Physical Society (1926-1948), 1948