Point defects in langatate crystals
- 28 March 2009
- journal article
- Published by Pleiades Publishing Ltd in Crystallography Reports
- Vol. 54 (2) , 279-282
Abstract
Langatate crystals of the general composition La3(Ga0.5Ta0.5)Ga5O14, grown by the Czochralski method, have been investigated by neutron diffraction (single crystals) and X-ray diffraction (ground single crystals). The crystals were grown in an atmosphere of 99% Ar + 1% O2 in the Y54° direction (rotation by 54° with respect to the y axis), without subsequent annealing (orange crystal) or with vacuum annealing (colorless crystal). It is established that colorless crystals have a higher gallium content and, therefore, a larger number of oxygen vacancies in comparison with colored crystals; this is a possible reason for their lower microhardness.Keywords
This publication has 6 references indexed in Scilit:
- A short history of SHELXActa Crystallographica Section A Foundations of Crystallography, 2007
- X-ray diffraction study of La3Ga5.5Ta0.5O14 and La3Ga5.5Nb0.5O14 langasite-type single crystalsInorganic Materials, 2005
- A family of langasite: growth and structureJournal of Crystal Growth, 2005
- Elastic and piezoelectric properties of La/sub 3/Ga/sub 5/SiO/sub 14/ and La/sub 3/Ga/sub 5.5/Ta/sub 0.5/O/sub 14/: an application of resonant ultrasound spectroscopyIEEE Transactions on Ultrasonics, Ferroelectrics, and Frequency Control, 2002
- Crystal Growth and Structural Characterization of New Piezoelectric Material La3Ta0.5Ga5.5O14Japanese Journal of Applied Physics, 1997
- Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenidesActa Crystallographica Section A, 1976