Failure analysis of one peculiar ‘Yin-Yang’ corrosion morphology on heat exchanger tubes in purified terephthalic acid (PTA) dryer
Authors:
- Yi GongYGYi Gong
- Zhen-Guo YangZYZhen-Guo Yang
- Xin-Hao MengXMXin-Hao Meng
- 1 July 2013
- journal article
- Published by Elsevier in Engineering Failure Analysis
- Vol. 31, 203-210
Abstract
No abstract availableKeywords
This publication has 13 references indexed in Scilit:
- Impact Simulation on Ductile Metal Pipe with Polymer Coating by a Coupled Finite Element and Meshfree MethodJournal of Failure Analysis and Prevention, 2012
- Heat Strength Evaluation and Microstructures Observation of the Welded Joints of One China-Made T91 SteelJournal of Materials Engineering and Performance, 2011
- Acidic/caustic alternating corrosion on carbon steel pipes in heat exchanger of ethylene plantMaterials and Corrosion, 2011
- Failure analysis of leakage on titanium tubes within heat exchangers in a nuclear power plant. Part II: Mechanical degradationMaterials and Corrosion, 2011
- Failure analysis of leakage on titanium tubes within heat exchangers in a nuclear power plant. Part I: Electrochemical corrosionMaterials and Corrosion, 2011
- Corrosion evaluation of one dry desulfurization equipment – Circulating fluidized bed boilerMaterials & Design (1980-2015), 2011
- Assessment of creep rupture properties for dissimilar steels welded joints between T92 and HR3CFatigue & Fracture of Engineering Materials & Structures, 2011
- Failure analysis of bursting on the inner pipe of a jacketed pipe in a tubular heat exchangerMaterials & Design (1980-2015), 2010
- Failure investigation of heat exchanger plates due to pitting corrosionEngineering Failure Analysis, 2010
- Anaerobic–aerobic treatment of purified terephthalic acid (PTA) effluent; a techno-economic alternative to two-stage aerobic processJournal of Environmental Management, 2007