Microstructure and Corrosion Resistance of Sn-3Ag-0.5Cu-xBi Solders
Authors:
- Michaela HalmanováMHMichaela Halmanová
- Ivona ČerničkováIČIvona Černičková
- Patrícia DanišovičováPDPatrícia Danišovičová
- Patrik ŠulhánekPŠPatrik Šulhánek
- Marián DrienovskýMDMarián Drienovský
- Xabier Zubizarreta CuerdaXCXabier Zubizarreta Cuerda
- Róbert HavlíkRHRóbert Havlík
- Libor ĎuriškaLĎLibor Ďuriška
- Marián PalcutMarián Palcut
Open Access
- 17 August 2026
- journal article
- research article
- Published by MDPI AG in Technologies
- Vol. 14 (8) , 509
Abstract
Sn-3Ag-0.5Cu-xBi alloys (SAC305-xBi) represent promising lead-free alternatives for low-temperature soldering. Low Bi concentrations can strengthen SAC-based solders through solid-solution strengthening, refining β–Sn grains and transforming needle-like Ag3Sn phases into equiaxed morphologies. However, excessive Bi alloying may induce precipitation of brittle Bi particles, cause microstructural instability and interfacial degradation, thereby weakening the solder joint performance. As such, the concentration of Bi in the SAC305 alloys should be carefully controlled. In this work, the microstructure and corrosion behavior of Sn-3Ag-0.5Cu-xBi solder alloys (SAC305-xBi, where x = 0, 1, 2 and 4 wt. %) were investigated. Attention has been paid to the influence of low Bi concentration on the microstructure, morphology, and chemical composition of the phases present in the solder alloys before and after corrosion exposure. The alloys were prepared by induction melting of Sn, Ag, Cu and Bi lumps under Ar gas. The microstructure of the SAC305 and SAC305-1Bi alloys represented a hypoeutectic microstructure with dendritic (Sn) grains and the ternary eutectic, consisting of (Sn), Cu6Sn5 and Ag3Sn, located in inter-dendritic regions. In the SAC305-2Bi and SAC305-4Bi alloys, a segregation of (Bi) particles was observed in addition to dendritic (Sn) and ternary eutectic. The (Bi) particles were located at the (Sn)Ag3Sn interface in the inter-dendritic spaces of the (Sn) solid solution. The corrosion resistance of the as-cast alloys was studied in aqueous NaCl electrolyte (3.5 wt. %) using electrochemical methods. Open circuit potentials of the alloys were found to increase with increasing concentration of Bi. The highest corrosion current was found for the SAC305-1Bi alloy. It was observed that micro-galvanic cells at the Sn-Ag3Sn interface were the initiating factors of corrosion in the SAC305-1Bi alloy. The corrosion activity of the SAC305-1Bi alloy is related to the high density of fine Ag3Sn particles. The higher fraction of Ag3Sn particles provided a dense network of local galvanic interaction sites, leading to the acceleration of the corrosion rate. The presence of discrete Bi precipitates in the SAC305-2Bi and SAC305-4Bi alloys, on the other hand, partially reduced the risk of galvanic corrosion. Since Bi has a higher standard electrode potential compared to Sn, the Bi/Ag3Sn and Bi/Cu6Sn5 couples were less prone to corrosion. The corrosion mechanism of the SAC305-xBi alloys is discussed, and results are compared to previously studied SAC-Bi alloys.Keywords
Funding Information
- European Commission (09I04-03-V02-00046)
This publication has 41 references indexed in Scilit:
- Microstructure, corrosion and mechanical properties of Sn–3.0Ag–0.5Cu solder alloy aged at 150 °CJournal of Materials Science: Materials in Electronics, 2025
- Bismuth addition affecting the microstructure evolution and anti-corrosion performance of Sn-3.0Ag-0.5Cu-xBi solder alloyJournal of Materials Science: Materials in Electronics, 2024
- Role of bismuth in the mechanical and corrosion properties of Cu/Sn-3.0Ag-0.5Cu/Cu solder lap jointsJournal of Materials Science: Materials in Electronics, 2024
- Insight into influence of temperature on electrochemical corrosion behavior of SAC305 tin-based solder alloy in NaCl solutionJournal of Materials Science: Materials in Electronics, 2023
- Corrosion behavior of Sn-based lead-free solder alloys: a reviewJournal of Materials Science: Materials in Electronics, 2020
- The reliability of lead-free solder joint subjected to special environment: a reviewJournal of Materials Science: Materials in Electronics, 2019
- Precipitation and coarsening of bismuth plates in Sn–Ag–Cu–Bi and Sn–Cu–Ni–Bi solder jointsJournal of Materials Science: Materials in Electronics, 2018
- Effect of microstructure and Ag3Sn intermetallic compounds on corrosion behavior of Sn–3.0Ag–0.5Cu lead-free solderJournal of Materials Science: Materials in Electronics, 2014
- Development of Sn–Ag–Cu and Sn–Ag–Cu–X alloys for Pb-free electronic solder applicationsJournal of Materials Science: Materials in Electronics, 2006
- Tin-silver-copper eutectic temperature and compositionMetallurgical and Materials Transactions A, 2000