Stabilization of the phosphatic wastes using high calcium ash in Jordan
- 1 November 2008
- journal article
- Published by Canadian Science Publishing in Canadian Journal of Civil Engineering
- Vol. 35 (11) , 1193-1199
Abstract
A significant amount of phosphatic waste and phosphatic overburden soils are stockpiled in the Al-Rusaifa area of Jordan. Research was completed on stabilizing this waste by mixing it with limy ash that was produced by the direct combustion of bituminous limestone. Doing so minimizes the environmental impact of the huge amount of phosphatic waste, and produces a product that can be used in various construction projects like earth works, pavement works, production of masonry blocks and curbstones. A variety of laboratory tests were completed to determine the suitability of the stabilized waste for these different uses. The S2 ash was produced by the direct combustion of bituminous limestone at 950 °C while the S3 ash was produced at 525 °C. Tests showed that the unconfined compressive strength of the parent phosphatic waste was raised from 1.5 kg/cm2 to 28.8 kg/cm2 for the S2 and to 22.4 kg/cm2 for the S3 ash treated samples. The new results were obtained despite a decrease in the maximum dry density to 1.47 g/cm3 when compared to 1.89 g/cm3 of the original untreated phosphatic waste. The soaked California bearing ratio was raised from 2.4% to 120%. The tests confirmed the suitability of the stabilized waste for a variety of construction applications.Keywords
This publication has 4 references indexed in Scilit:
- Utilization of bituminous limestone ash from EL-LAJJUN area for engineering applicationsActa Geotechnica, 2008
- Utilization of fly ash for stabilization/solidification of heavy metal contaminated soilsEngineering Geology, 2003
- Development of stabilisation and solidification in lime–clay mixesGéotechnique, 2001
- Stabilization Characteristics of Clays Using Class C Fly AshTransportation Research Record: Journal of the Transportation Research Board, 1998