Abstract
Fouling deposition and localized corrosion on the heat‐transfer surfaces of the stainless steel equipments often simultaneously exist, which can introduce additional thermal resistance to heat‐transfer and damage heat‐transfer surfaces. It is a good anticorrosion way to coat a barrier layer of certain materials on the metal surface. In this article, the TiO2 coatings with nanoscale thicknesses were obtained by liquid‐phase deposition method on the substrates of AISI304 stainless steel (ASS). The coating thickness, surface roughness, surface morphology, crystal phase, and chemical element were characterized with the film thickness measuring instrument, roughmeter, atomic force microscopy, field emission scanning electron microscopy, X‐ray diffraction, and energy‐dispersive X‐ray spectroscopy analyzer, respectively. Corrosion behavior of the TiO2 coatings was evaluated by potentiodynamic polarization, cyclic voltammograms scanning, and electrochemical impedance spectroscopy tests with the mixed corrosion solution composed of 3.5 wt. % NaCl and 0.05 M NaOH. It is shown that the TiO2 coating is composed of the nanoparticles with smooth, crack‐free, dense, and uniform surface topography; the roughness of coating surface increases slightly compared with that of the polished ASS substrate. The anatase‐phase TiO2 coatings are obtained when sintering temperature being varied from 573.15 to 923.15 K and exhibit better anticorrosion behavior compared with ASS surfaces. The corrosion current density decreases and the polarization resistance increases with the increase of the coating thickness. The corrosion resistance of the TiO2 coatings deteriorates with the increase of the corrosion time. The capacitance and the resistance of the corrosion product layer between the interface of the ASS substrate and the TiO2 coating are found after the corrosion time of 240 h. A corrosion model was introduced, and a possible new explanation on the anticorrosion mechanisms of the TiO2 coating was also analyzed. The corrosion mechanism of the TiO2 coating might comply with the multistage corrosion process. © 2011 American Institute of Chemical Engineers AIChE J, 58: 1907–1920, 2012Keywords
This publication has 49 references indexed in Scilit:
- Pool boiling fouling and corrosion properties on liquid‐phase‐deposition TiO2 coatings with copper substrateAIChE Journal, 2010
- Pitting Corrosion of Bare Stainless Steel 304 under Chloride Solution DropletsJournal of the Electrochemical Society, 2010
- Corrosion protection of mild steel by applying TiO2 nanoparticle coating via sol-gel methodProtection of Metals and Physical Chemistry of Surfaces, 2009
- Antifouling and enhancing pool boiling by TiO2 coating surface in nanometer scale thicknessAIChE Journal, 2007
- Enhancing flow boiling and antifouling with nanometer titanium dioxide coating surfacesAIChE Journal, 2007
- TiO2 photocatalysts deposited on fiber substrates by liquid phase depositionJournal of Photochemistry and Photobiology A: Chemistry, 2004
- Thin TiO2 Films Prepared by Low Pressure Chemical Vapor DepositionJournal of the Electrochemical Society, 1993
- Fouling Due to Corrosion Products Formed on a Heat Transfer SurfaceJournal of Heat Transfer, 1987
- The Equivalent Conductance of the Hexafluorocomplexes of Group IV (Si, Ge, Sn, Ti, Zr, Hf)1Journal of the American Chemical Society, 1960
- Equilibria in the System Boron Trifluoride—Water at 25°Journal of the American Chemical Society, 1951