Effects of heating rate and temperature on product distribution of poly-lactic acid and poly-3-hydroxybutyrate-co-3-hydroxyhexanoate
Open Access
- 20 December 2022
- journal article
- research article
- Published by Springer Nature in Journal of Material Cycles and Waste Management
- Vol. 25 (2) , 650-661
Abstract
In this study, poly-lactic acid (PLA) and poly-3-hydroxybutyrate-co-3-hydroxyhexanoate (PHBH) were pyrolyzed at various temperatures (300, 350, 400, 500, 600, and 700 °C) and heating rates (5, 10, 20, 30, and 40 °C min−1) using a pyrolysis–gas chromatograph/mass spectrometer (Py–GC/MS). The results revealed that the main pyrolysis products of PLA were acetaldehyde, lactide (including meso-lactide and d-, l-lactide), and oligomers. Crotonic acid and its oligomers accounted for most of the PHBH pyrolyzates. The pyrolysis temperature significantly correlated with the product distribution, but the heating rate had a small effect on the product distribution. Lactide and crotonic acid were two kinds of high-value chemicals, and their highest yields were obtained at 400 and 600 °C with 29.7 and 72.6 area %, respectively. Secondary reactions could not be neglected at 700 °C, and acetaldehyde and crotonic acid decreased to 65.0 and 69.6 area %, respectively. These results imply that pyrolyzate selectivity can be controlled by temperature management during pyrolysis.Keywords
Funding Information
- Environment Research and Technology Development Fund (JPMEERF21511901)
This publication has 55 references indexed in Scilit:
- Thermal degradation behaviors of polyethylene and polypropylene. Part I: Pyrolysis kinetics and mechanismsEnergy Conversion and Management, 2010
- Chemical recycling of polyhydroxyalkanoates as a method towards sustainable developmentBiotechnology Journal, 2010
- Thermal degradation kinetics of g-HA/PLA compositeThermochimica Acta, 2009
- Anhydride production as an additional mechanism of poly(3‐hydroxybutyrate) pyrolysisJournal of Applied Polymer Science, 2008
- Effects of chain end structures on pyrolysis of poly(-lactic acid) containing tin atomsPolymer Degradation and Stability, 2004
- The determination of activation energy from linear heating rate experiments: a comparison of the accuracy of isoconversion methodsThermochimica Acta, 2003
- Thermal degradation of poly(3‐hydroxybutyrate) and poly(3‐hydroxybutyrate‐co‐3‐hydroxyvalerate) as studied by TG, TG–FTIR, and Py–GC/MSJournal of Applied Polymer Science, 2003
- Estimation of activation energy by isoconversion methodsThermochimica Acta, 1992
- Applicability of the master plots in kinetic analysis of non-isothermal dataThermochimica Acta, 1989
- Variation of peak temperature with heating rate in differential thermal analysisJournal of Research of the National Bureau of Standards, 1956