Simultaneous Temperature Measurement of Wafers in Chemical Mechanical Polishing of Silicon Dioxide Layer
Authors:
- Fumitoshi SugimotoFSFumitoshi Sugimoto
- Yoshihiro ArimotoYAYoshihiro Arimoto
- Takashi ItoTITakashi Ito
- 1 December 1995
- journal article
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 34 (12R) , 6314-6320
Abstract
The wafer temperature in chemical mechanical polishing (CMP) of silicon dioxide layers was measured. When the temperatures of both the polishing slurry and the polishing pad were controlled at 8° C, the measured wafer temperatures were 10-20° C. The temperature distribution affected the thickness of the polished oxide layer. When the wafer temperature was high, the oxide layer removal rate increased because of the increased reaction of the slurry with the oxide layer. It was clear that there was a linear relationship between the measured wafer temperature and the oxide layer removal rate. The effects of grooving several typical polishing pads for oxide layer polishing were investigated. It was found that grooves on the pad increased the uniformity of the removal of the oxide layer from the wafer.Keywords
This publication has 5 references indexed in Scilit:
- Mirror Polishing of Si Wafers (3rd Report)Journal of the Japan Society for Precision Engineering, 1992
- A Two‐Dimensional Process Model for Chemimechanical Polish PlanarizationJournal of the Electrochemical Society, 1991
- Application of Chemical Mechanical Polishing to the Fabrication of VLSI Circuit InterconnectionsJournal of the Electrochemical Society, 1991
- Planarization of dielectrics used in the manufacture of very-large-scale integrated circuitsThin Solid Films, 1990
- Characterization of Microdeformation and Crystal Defects in Silicon Wafer SurfacesJournal of the Electrochemical Society, 1983