Acidizing Sandstone Reservoirs Using HF and Formic Acids

Authors:

Abstract
Mud acid, which is composed of HCl and HF, is commonly used to remove the formation damage in sandstone reservoirs. However, many problems are associated with HCl acid, especially at high temperatures. In this study, formic acid was used to remove carbonate minerals as a preflush and with the main HF stage. A series of formic acid and HF mixtures with different ratios and concentrations were tested. Sandstone cores featured by different minerologies with dimensions of 1.5 in. x 6 in. were used in the coreflood experiments, which were run at a flow rate of 5 cm3/min and temperatures from 77 to 350°F. The cores were analyzed by CT scan before and after the acidizing to investigate the effect of the acid. The core effluent samples were analyzed to determine concentrations of Ca, Mg, Fe, Si, and Al by ICP. 19F NMR was utilized to follow the reaction kinetics and products. Zeta potentials of clay particles (kaolinite, illite, and chlorite) were measured in various acid solutions Formic acid (9 wt%) damaged sandstone cores. Zeta potential measurements indicated that formic acid can trigger fines flocculation. Addition of 5 wt% ammonium chloride helps to shield negative charges on clay surface. Analysis of core effluent samples indicated that there was CaF2 precipitate in the core when a small volume of preflush was used. Coreflood tests highlighted that formic acid/HF caused loss of core permeability. This paper will discuss the detailed chemical reactions occurred within cores and were followed by chemical analysis of core effluent samples and 19F NMR. Secondary reaction between clay minerals and HF became faster at higher temperature, and decreased the ratio of Si/Al. It was also found that different clay minerals react with HF offering very different concentrations of Al and Si in spent acid.

This publication has 20 references indexed in Scilit: