Microstructural stability of thermal shayed WC–Co composite coatings in oxidising atmospheres at 450°C
Authors:
- D. NolanDND. Nolan
- P. MercerPMP. Mercer
- M. SamandiMSM. Samandi
- 1 January 1998
- journal article
- Published by SAGE Publications in Surface Engineering
- Vol. 14 (2) , 124-128
Abstract
The present work stems from a development programme considering the use of WC–Co thermal spraycoatings in galvanising applications. In such applications, service conditions include exposure to air at 450°C. It is generally accepted that WC–Co composites do not oxidise significantly in air at temperatures below 500°C. However, the present results show significant oxidation of such coatingsat 450°C in air and in contact with a molten galvanising alloy. There appear to be two simultaneous oxidation reactions occurring, with WO3 forming from the tungsten carbide and tungsten phases and CoWO4 derived from the β-Co and cobalt containing carbide phases.Keywords
This publication has 4 references indexed in Scilit:
- Revealing true porosity in WC-Co thermal spray coatingsJournal of Thermal Spray Technology, 1997
- Formation of an amorphous phase in thermally sprayed WC-CoJournal of Thermal Spray Technology, 1996
- Microstructure and hydroabrasive wear behaviour of high velocity oxy-fuel thermally sprayed WCCo(Cr) coatingsSurface and Coatings Technology, 1993
- Thermally sprayed coating systems for surface protection and clearance control applications in aero enginesSurface and Coatings Technology, 1990