Abstract
The performance of four 1.5 mm thick high-density polyethylene (HDPE) geomembranes (GMBs) (denoted MxA-15, MxC-15, MyE-15, and MyEW-15) immersed in a brine solution with 200,000 ppm total dissolved solids and a pH = 8.7 is presented for 4 years. Accelerated ageing experiments were conducted at 40, 65, 75, and 85°C for 4 years. It is shown that neither the Std-OIT nor HP-OIT had reached a residual value before physical degradation was observed, suggesting that the traditional three-stage concept for degradation did not apply when based on the values obtained (as is usual) through the entire GMB thickness. The time to nominal failure, based on a reduction of 50% of the initial value, was less than 4 years for all GMBs at temperatures ≥ 65°C. However, using the time at which the stress crack resistance (SCR), obtained from the single point notched constant tensile load (SP-NCTL) test, decreased to 50% of the minimum requirements of GRI-GM13, the times to nominal failure are greater than 20 years for at T ≤ 65°C for MyE-15.Keywords
This publication has 21 references indexed in Scilit:
- Effect of high temperatures on the physical and mechanical properties of HDPE geomembranes in airGeosynthetics International, 2015
- Effect of leachate composition on the long-term performance of a HDPE geomembraneGeotextiles and Geomembranes, 2014
- Degradation behaviour of HDPE geomembranes with high and low initial high-pressure oxidative induction timeGeotextiles and Geomembranes, 2014
- Antioxidant depletion of HDPE geomembrane with sand protection layerGeosynthetics International, 2013
- Heat extraction methods from salinity-gradient solar ponds and introduction of a novel system of heat extraction for improved efficiencySolar Energy, 2011
- Diffusion modelling of OIT depletion from HDPE geomembrane in landfill applicationsGeosynthetics International, 2009
- Effect of acidic mine drainage on the polymer properties of an HDPE geomembraneGeosynthetics International, 2004
- Geomembranelinerdurability: Contributing factors and the status quo2003
- Oxidative resistance of high-density polyethylene geomembranesPolymer Degradation and Stability, 2003
- Antioxidant Depletion Lifetime in High Density Polyethylene GeomembranesJournal of Geotechnical and Geoenvironmental Engineering, 1998