The influence of aging on the fracture load of milled monolithic crowns
Authors:
Open Access
- 19 November 2022
- journal article
- research article
- Published by Springer Nature in BMC Oral Health
- Vol. 22 (1) , 1-9
Abstract
Background: This in-vitro study was conducted to assess the effect of aging on the fracture load of molar crowns fabricated with monolithic CAD/CAM materials. Methods: The crown restorations were produced from Cerasmart, Vita Enamic, and IPS e.max CAD blocks. Aging was applied to the 10 samples each of monolithic CAD/CAM materials (n = 10). Dual-axis chewing simulator (50 N, 1.1 Hz, lateral movement: 1 mm, mouth opening: 2 mm, 1,200,000 cycles) and thermocycling (± 5–55 °C, 6000 cycles) were applied as an aging procedure. 10 samples each of monolithic CAD/CAM materials without aging (n = 10) were considered the control group. 6 tested groups were obtained. Then, all samples were evaluated in a universal testing machine to determine the fracture loading values’. Results: There was not a statistically significant difference between the fracture load values before and after aging for all samples of Cerasmart, Vita Enamic, and IPS e.max CAD (p > 0.005). In a comparison of the monolithic materials together, a statistically significant difference was found between the fracture load values of IPS e.max CAD and Vita Enamic crowns before aging (p = 0.02). Also, Vita Enamic crowns (1978,71 ± 364,05 N) were found different from the IPS e.max CAD (p = 0.005) and Cerasmart crowns (p = 0.041) after aging. Conclusions: Dynamic aging with 1.200.000 cycles was found to have no effect to fracture loading on milled Cerasmart, Vita Enamic, and IPS e.max CAD monolithic crowns.Keywords
All Related Versions
This publication has 39 references indexed in Scilit:
- Chair-side generated posterior lithium disilicate crowns after 4 yearsClinical Oral Investigations, 2012
- Wear performance of dental ceramics after grinding and polishing treatmentsJournal of the Mechanical Behavior of Biomedical Materials, 2012
- Wear performance of substructure ceramics and veneering porcelainsDental Materials, 2011
- In vitro fatigue resistance of CAD/CAM composite resin and ceramic posterior occlusal veneersThe Journal of Prosthetic Dentistry, 2010
- Dynamic fatigue and fracture resistance of non-retentive all-ceramic full-coverage molar restorations. Influence of ceramic material and preparation designDental Materials, 2010
- Effect of Ultrasonic Versus Manual Cementation on the Fracture Strength of Resin Composite LaminatesOperative Dentistry, 2009
- Approach for valuating the significance of laboratory simulationJournal of Dentistry, 2008
- Influence of stress simulation parameters on the fracture strength of all-ceramic fixed-partial denturesDental Materials, 2006
- Wear of composite resin veneering materials in a dual‐axis chewing simulatorJournal of Oral Rehabilitation, 1999
- An artificial oral environment for testing dental materialsIEEE Transactions on Biomedical Engineering, 1991