Abstract
The different parameters used for the photoactivation process provide changes in the degree of conversion (DC%) and temperature rise (TR) of the composite resins. Thus, the purpose of this study was to evaluate the DC (%) and TR of the microhybrid composite resin photoactivated by a new generation LED. For the KBr pellet technique, the composite resin was placed into a metallic mould (1-mm thickness and 4-mm diameter) and photoactivated as follows: continuous LED LCU with different power density values (50–1000 mW/cm2). The measurements for the DC (%) were made in a FTIR Spectrometer Bomen (model MB-102, Quebec-Canada). The spectroscopy (FTIR) spectra for both uncured and cured samples were analyzed using an accessory for the diffuse reflectance. The measurements were recorded in the absorbance operating under the following conditions: 32 scans, 4-cm−1 resolution, and a 300 to 4000-cm−1 wavelength. The percentage of unreacted carbon-carbon double bonds (% C=C) was determined from the ratio of the absorbance intensities of aliphatic C=C (peak at 1638 cm−1) against an internal standard before and after the curing of the specimen: aromatic C-C (peak at 1608 cm−1). For the TR, the samples were made in a metallic mould (2-mm thickness and 4-mm diameter) and photoactivated during 5, 10, and 20 s. The thermocouple was attached to the multimeter to allow the temperature readings. The DC (%) and TR were calculated by the standard technique and submitted to ANOVA and Tukey’s test (p < 0.05). The degree of conversion values varied from 35.0 (±1.3) to 45.0 (±2.4) for 5 s, 45.0 (±1.3) to 55.0 (±2.4) for 10 s, and 47.0 (±1.3) to 52.0 (±2.4) for 20 s. For the TR, the values ranged from 0.3 (±0.01) to 5.4 (±0.11)°C for 5 s, from 0.5 (±0.02) to 9.3 (±0.28)°C for 10 s, and from 1.0 (±0.06) to 15.0 (±0.95)°C for 20 s. The power densities and irradiation times showed a significant effect on the degree of conversion and temperature rise.Keywords
This publication has 21 references indexed in Scilit:
- Influence of photoactivation method on conversion, mechanical properties, degradation in ethanol and contraction stress of resin-based materialsJournal of Dentistry, 2005
- The effect of different light-curing units on fatigue behavior and degree of conversion of a resin compositeDental Materials, 2005
- Temperature rise during polymerization of light‐activated resin compositesJournal of Oral Rehabilitation, 1998
- Clinical and histological evaluation of thermal injury thresholds in human teeth: a preliminary studyJournal of Oral Rehabilitation, 1997
- Effect of Light Intensity on Polymerization of Light-cured Composite ResinsDental Materials Journal, 1994
- Measurement of temperature generated by visible-light-cure lamps in an in vitro modelDental Materials, 1989
- Temperature rise during polymerization of visible light-activated composite resinsDental Materials, 1988
- Correlation between hardness and degree of conversion during the setting reaction of unfilled dental restorative resinsDental Materials, 1985
- Factors Affecting the Depth of Cure of UV -polymerized CompositesJournal of Dental Research, 1980
- Pulp response to externally applied heatOral Surgery, Oral Medicine, Oral Pathology, 1965