Study on Microstructure and Mechanical Properties of Laser Welded Dissimilar Joint of P91 Steel and INCOLOY 800HT Nickel Alloy
Open Access
Abstract
This investigation attempts to explore the weld characteristics of a laser welded dissimilar joint of ferritic/martensitic 9Cr-1Mo-V-Nb (P91) steel and Incoloy 800HT austenitic nickel alloy. This dissimilar joint is essential in power generating nuclear and thermal plants operating at 600–650 °C. In such critical operating conditions, it is essential for a dissimilar joint to preserve its characteristics and be free from any kind of defect. The difference between the physical properties of P91 and Incoloy 800HT makes their weldability challenging. Thus, the need for detailed characterization of this dissimilar weld arises. The present work intends to explore the usage of an unconventional welding process (i.e., laser beam welding) and its effect on the joint’s characteristics. The single-pass laser welding technique was employed to obtain maximum penetration through the keyhole mode. The welded joint morphology and mechanical properties were studied in as-welded (AW) and post-weld heat treatment (PWHT) conditions. The macro-optical examination shows the complete penetrations with no inclusion and porosities in the weld. The microstructural study was done in order to observe the precipitation and segregation of elements in dendritic and interface regions. Solidification cracks were observed in the weld fusion zone, confirming the susceptibility of Incoloy 800HT to such cracks due to a mismatch between the melting point and thermal conductivity of the base metals. Failure from base metal was observed in tensile test results of standard AW specimen with a yield stress of 265 MPa, and after PWHT, the value increased to 297 MPa. The peak hardness of 391 HV was observed in the P91 coarse grain heat-affected zone (CGHAZ), and PWHT confirmed the reduction in hardness. The impact toughness results that were obtained were inadequate, as the maximum value of impact toughness was obtained for AW P91 heat-affected zone (HAZ) 108 J and the minimum for PWHT Incoloy 800HT HAZ 45 J. Thus, difficulty in obtaining a dissimilar joint with Incoloy 800HT using the laser beam welding technique was observed due to its susceptibility to solidification cracking.Keywords
This publication has 51 references indexed in Scilit:
- Failure analysis of Incoloy 800HT pipe at high temperatureEngineering Failure Analysis, 2013
- Effect of Activated Flux on the Microstructure, Mechanical Properties, and Residual Stresses of Modified 9Cr-1Mo Steel Weld JointsMetallurgical and Materials Transactions B, 2011
- Characterization of microstructures and mechanical properties of Inconel 617/310 stainless steel dissimilar weldsMaterials Characterization, 2011
- The impact of welding on the creep properties of advanced 9–12% Cr steelsTransactions of the Indian Institute of Metals, 2010
- Microstructure and Mechanical Properties of 9Cr-1Mo Steel Weld Fusion Zones as a Function of Weld Metal CompositionJournal of Materials Engineering and Performance, 2009
- Ferritic/martensitic steels for advanced nuclear reactorsTransactions of the Indian Institute of Metals, 2009
- Microstructural changes and mechanical properties of Incoloy 800 after 15 years serviceMaterials Characterization, 2009
- Microstructural features of dissimilar welds between 316LN austenitic stainless steel and alloy 800Materials Science and Engineering: A, 2000
- Effect of aging on the microstructure and tensile properties of an alloy 800/9Cr-1Mo steel jointInternational Journal of Pressure Vessels and Piping, 1995
- A phase diagram approach to study liquation cracking in alloy 718Metallurgical Transactions A, 1991