Fatigue behavior of thin-walled grade 2 titanium samples processed by selective laser melting. Application to life prediction of porous titanium implants
Authors:
- P. LipinskiPLP. Lipinski
- A. BarbasABA. Barbas
- A.-S. BonnetABA.-S. Bonnet
- 1 December 2013
- journal article
- Published by Elsevier in Journal of the Mechanical Behavior of Biomedical Materials
- Vol. 28, 274-290
Abstract
No abstract availableKeywords
This publication has 14 references indexed in Scilit:
- Accuracy of medical models made by additive manufacturing (rapid manufacturing)Journal of Cranio-Maxillofacial Surgery, 2013
- On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: Fatigue resistance and crack growth performanceInternational Journal of Fatigue, 2013
- Surface Finish after Laser Metal DepositionPhysics Procedia, 2013
- Fatigue of Ti-6Al-4V2012
- Development and mechanical characterization of porous titanium bone substitutesJournal of the Mechanical Behavior of Biomedical Materials, 2012
- Additive manufactured AlSi10Mg samples using Selective Laser Melting (SLM): Microstructure, high cycle fatigue, and fracture behaviorMaterials & Design (1980-2015), 2012
- Bioactive Ti metal analogous to human cancellous bone: Fabrication by selective laser melting and chemical treatmentsActa Biomaterialia, 2011
- Net shaped high performance oxide ceramic parts by selective laser meltingPhysics Procedia, 2010
- Structural, mechanical and in vitro characterization of individually structured Ti–6Al–4V produced by direct laser formingBiomaterials, 2006
- The long-term clinical relevance of calcar atrophy caused by stress shielding in total hip arthroplastyThe Journal of Arthroplasty, 2004