The investigation of structural and morphological changes after the chlorination of rubber surfaces
Authors:
- 12 March 1990
- journal article
- research article
- Published by Wiley in Die Angewandte Makromolekulare Chemie
- Vol. 176 (1) , 161-172
Abstract
The samples of vulcanized rubber compounds with natural rubber (NR) and styrene‐butadiene rubber (SBR) were prepared. The surface chlorination of samples was performed by immersion of strips in aqueous solution of sodium hypochlorite and in hydrochloric acid in dependence of time and in temperature range from 20 °C to 80°C. The changes of chemical structures, thermal stability and morphological properties of chlorinated vulcanizates were recorded by IR‐FMIR spectroscopy, differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), wide angle X‐ray diffraction (WAXD) and scanning electron microscopy (SEM). Extremely heterogeneous complex mechanisms of chlorination and parallel degradation processes in dependence on time and temperature above all were indicated and compared to NR and SBR vulcanizates. At higher temperatures the structural changes in elastomeric matrix in connection with selective separation and surface migration of multicomponent filler due to agressive media were observed.Keywords
This publication has 12 references indexed in Scilit:
- Ageing and Weathering of Mica-SBR CompositesJournal of Elastomers & Plastics, 1988
- Structure and stability of halogenated polymers: Part 2—Chain-chlorinated polystyrenePolymer Degradation and Stability, 1987
- Structure and stability of halogenated polymers: Part 1—Ring-chlorinated polystyrenePolymer Degradation and Stability, 1987
- Initial stage of the chlorination of natural rubberEuropean Polymer Journal, 1985
- Thermal stability, fractionation, and chemical modification of chlorinated rubbers. I. Infrared and 13C‐NMR study of the structure of chlorinated natural rubber modified under various experimental conditionsJournal of Applied Polymer Science, 1984
- Surface Modification of Elastomers for BondingThe Journal of Adhesion, 1983
- Bromine Terminated Liquid Polybutadiene as a Solventless, Room-Temperature Adhesive SystemRubber Chemistry and Technology, 1980
- Investigations on poly(vinyl chloride). II. Pyrolysis of chlorinated polybutadienes as model compounds for poly(vinyl chloride)Journal of Polymer Science: Polymer Chemistry Edition, 1975
- Thermal degradation of chlorinated rubber: Evidence for an alternative cyclic structure for chlorinated rubberJournal of Polymer Science: Polymer Chemistry Edition, 1974
- Chlorination of Rubber and Some Products of Its Partial ChlorinationRubber Chemistry and Technology, 1956