Bending moments of zirconia and titanium implant abutments supporting all‐ceramic crowns after aging
- 4 June 2013
- journal article
- Published by Wiley in Clinical Oral Implants Research
- Vol. 25 (1) , 74-81
Abstract
Objectives: To test the fracture load and fracture patterns of zirconia abutments restored with all‐ceramic crowns after fatigue loading, exhibiting internal and external implant–abutment connections as compared to restored and internally fixed titanium abutments.Materials and methods: A master abutment was used for the customization of 5 groups of zirconia abutments to a similar shape (test). The groups differed according to their implant–abutment connections: one‐piece internal connection (BL; Straumann Bonelevel), two‐piece internal connection (RS; Nobel Biocare ReplaceSelect), external connection (B; Branemark MkIII), two‐piece internal connection (SP, Straumann StandardPlus) and one‐piece internal connection (A; Astra Tech AB OsseoSpeed). Titanium abutments with internal implant–abutment connection (T; Straumann Bonelevel) served as control group. In each group, 12 abutments were fabricated, mounted to the respective implants and restored with glass–ceramic crowns. All samples were embedded in acrylic holders (ISO‐Norm 14801). After aging by means of thermocycling in a chewing simulator, static load was applied until failure (ISO‐Norm 14801). Fracture load was analyzed by calculating the bending moments. Values of all groups were compared with one‐way ANOVA followed by Scheffé post hoc test (P‐value<0.05). Failure mode was analyzed descriptively.Results: The mean bending moments were 464.9 ± 106.6 N cm (BL), 581.8 ± 172.8 N cm (RS), 556.7 ± 128.4 N cm (B), 605.4 ± 54.7 N cm (SP), 216.4 ± 90.0 N cm (A) and 1042.0 ± 86.8 N cm (T). No difference of mean bending moments was found between groups BL, RS, B and SP. Test group A exhibited significantly lower mean bending moment than the other test groups. Control group T had significantly higher bending moments than all test groups. Failure due to fracture of the abutment and/or crown occurred in the test groups. In groups BL and A, fractures were located in the internal part of the connection, whereas in groups RS and SP, a partial deformation of the implant components occurred and cracks and fractures of the zirconia abutment were detected.Conclusion: The differently connected zirconia abutments exhibited similar bending moments with the exception of one group. Hence, the type of connection only had a minor effect on the stability of restored zirconia abutments. In general, restored titanium abutments exhibited the highest bending moments.Keywords
This publication has 24 references indexed in Scilit:
- Systematic review of the survival rate and the incidence of biological, technical, and aesthetic complications of single crowns on implants reported in longitudinal studies with a mean follow‐up of 5 yearsClinical Oral Implants Research, 2012
- The effect of zirconia and titanium implant abutments on light reflection of the supporting soft tissuesClinical Oral Implants Research, 2011
- Influence of cyclic fatigue in water on the load-bearing capacity of dental bridges made of zirconiaActa Biomaterialia, 2008
- A systematic review of the 5‐year survival and complication rates of implant‐supported single crownsClinical Oral Implants Research, 2007
- Fracture resistance of single‐tooth implant‐supported all‐ceramic restorations after exposure to the artificial mouthJournal of Oral Rehabilitation, 2006
- Fracture resistance of single-tooth implant-supported all-ceramic restorations: An in vitro studyThe Journal of Prosthetic Dentistry, 2006
- What future for zirconia as a biomaterial?Biomaterials, 2006
- Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramicsDental Materials, 2004
- Fatigue resistance of two implant/abutment joint designsThe Journal of Prosthetic Dentistry, 2002
- Lifetime-limiting Strength Degradation from Contact Fatigue in Dental CeramicsJournal of Dental Research, 2000