The Effect of Compaction Method on the Expansion and Stability of Aluminium Foams
Authors:
- 26 September 2006
- journal article
- other
- Published by Wiley in Advanced Engineering Materials
- Vol. 8 (9) , 810-815
Abstract
The foam expansion and collapse behaviour for heat treated Al‐TiH2 precursors has been shown to be driven by the oxidation of the Al powder, which can, in moderation, improve the foam expansion and increase foam stability, and the premature loss of gas from the TiH2, which delays but decreases the foam expansion. The evidence presented indicates that as long as theoretical precursor densities > 99 % can be achieved, simultaneous heating and compaction are not required to achieve the best foaming behaviour. Instead, the oxygen or oxide content in the powder is critical and if the oxygen content in the atomised powder is in the range 0.3–0.4 wt.%, cold compaction is sufficient to produce foams which show expansions at least as good as those for precursors made by high cost hot working processes.Keywords
This publication has 7 references indexed in Scilit:
- Effect of Ceramic Particle Additions on Foam Expansion and Stability in Compacted Al‐TiH2 Powder PrecursorsAdvanced Engineering Materials, 2004
- Effects of TiB2 particle addition on the expansion, structure and mechanical properties of PM Al foamsScripta Materialia, 2004
- The decomposition behavior of as-received and oxidized TiH2 foaming-agent powderMaterials Science and Engineering: A, 2003
- The effect of TiH2 heat treatment on gas release and foaming in Al–TiH2 preformsScripta Materialia, 2002
- Effect of compaction density on foamability of Al–TiH2powder compactsPowder Metallurgy, 2002
- Manufacture, characterisation and application of cellular metals and metal foamsProgress in Materials Science, 2001
- A study of aluminium foam formation—kinetics and microstructureActa Materialia, 2000