Si 3 N 4 /BN fibrous monoliths were prepared with 4 wt% Y 2 O 3 added as a sintering aid to the Si 3 N 4 . Residual carbon, present in the billet before hot‐pressing, was shown to influence the final microstructure. The sintering aid glass, known to migrate into the BN cell boundaries during hot‐pressing, was not sufficient in quantity to prevent premature shear failure when samples were tested in flexure. Increasing the hot‐pressing temperature alleviated this problem. For flexure samples tested at 1400°C, fibrous monoliths fabricated with 4 wt% Y 2 O 3 demonstrated linear‐elastic loading behavior at a greater stress than fibrous monoliths fabricated with 6‐wt%‐Y 2 O 3 /2‐wt%‐Al 2 O 3 sintering aids.