Pb(Zr0.5,Ti0.5)O3 (PZT) thin films were deposited through chemical solution deposition (CSD) on Pt/Ti/SiO2/Si substrates by electric-field-assisted annealing (EFA-A). XRD relative intensities for the (001)&(100) planes of the PZT perovskite phase in films deposited by EFA-A increased with increasing applied electric field. However, the electrical properties of the resultant PZT thin films deposited by EFA-A could not be measured because of the relatively large cracks formed during EFA-A. Therefore, two additional processes were introduced to obtain (001)-oriented PZT films with good electrical properties. One of the processes was the deposition of PZT film with a PbO seeding layer by EFA-A and the other was the infiltration process after the deposition of films by EFA-A to heal the cracks formed by EFA-A. The results indicated that cracks caused by EFA-A could be infiltrated by post-annealing to show relatively good remanent polarization (Pr) and a large effective piezoelectric constant of d33 compared with those of the films deposited without EFA-A. The measured remanent polarization for the films with and without EFA-A were 12.5 µC/cm2 and 10.9 µC/cm2, respectively. In addition, the PZT film deposited with a PbO seeding layer by EFA-A also exhibited a larger effective d33 of 230 pC/N in comparison with the film deposited without EFA-A.