Thermo-Mechanical Reliability of Nano-Silver Sintered Joints versus Lead-Free Solder Joints for Attaching Large-Area Silicon Devices
Authors:
- 2 November 2010
- conference paper
- Published by SAE International in SAE International Journal of Advances and Current Practices in Mobility
- Vol. 1
Abstract
Nano-silver sintered bonding was carried out at 275°C and under 3MPa pressures, and soldering in a vacuum reflowing oven to reduce voiding. Both joints are subject to large shear stresses due to the mismatch in coefficients of thermal expansion (CTE) between the chip and the substrate. In this study, residual stresses in the chip-on-substrate assemblies were determined by measuring the bending curvatures of the bonded structures. An in-house optical setup measured the bending curvatures using a thin-film stress measurement technique. From the measured bending curvatures and the mechanical properties of the constituent materials, residual stresses were calculated. The thermo-mechanical reliabilities of both joining techniques were tested by thermal cycling. The chip assemblies were cycled between -40°C and 125°C (100 minutes of cycle time, 10 minutes of dwell time) and the changes in their bending curvatures were measured. Residual stresses were found to decrease with temperature cycling, which may be due to stress relaxation from creep or crack formation in the die-attach materials. Failure analysis of sintered nano-silver joints, eutectic Sn-3.5Ag solder (SAC305) joints and eutectic SnCu0.7Ni solder (SN100C) joints was performed by means of cross-sectioning and scanning electron microscopy (SEM) after 800 thermal cycles. For both solder materials with copper substrate, fatigue fracture started at the edge of the solder, and crack propagation across the solder joint was observed. No cracks were found at the joints between silicon and sintered nano-silver. The stress-relaxation behavior of all die-attach layers are hypothesized.Keywords
This publication has 11 references indexed in Scilit:
- Joint Reliability of Double-Side Packaged SiC Power Devices to a DBC Substrate with High Temperature Solders2008
- Tensile Behaviors and Ratcheting Effects of Partially Sintered Chip-Attachment Films of a Nanoscale Silver PasteJournal of Electronic Materials, 2008
- Thermomechanical Reliability of Low-Temperature Sintered Silver Die Attached SiC Power Device AssemblyIEEE Transactions on Device and Materials Reliability, 2006
- Nanoscale Silver Paste and its Sintering for Attaching Semiconductor Devices2006
- Three-dimensional packaging for power semiconductor devices and modulesIEEE Transactions on Advanced Packaging, 2005
- Reliability and Failure Analysis of Sn-Ag-Cu Solder Interconnections for PSGA Packages on Ni/Au Surface FinishIEEE Transactions on Device and Materials Reliability, 2004
- Power cycling reliability of IGBT power modules2002
- Modeling of elastic deformation of multilayers due to residual stresses and external bendingJournal of Applied Physics, 2002
- Solder joint fatigue models: review and applicability to chip scale packagesMicroelectronics Reliability, 2000
- Microstructure evolution of eutectic Sn-Ag solder jointsJournal of Electronic Materials, 1994