Experimental evaluations of the strength of silicon die by 3-point-bend versus Ball-on-Ring tests
Authors:
- 1 May 2008
- conference paper
- Published by Institute of Electrical and Electronics Engineers (IEEE) in 2008 11th Intersociety Conference on Thermal and Thermomechanical Phenomena in Electronic Systems
- No. 10879870,p. 687-694
Abstract
Silicon wafers and dies are single crystal in semiconductor applications which must withstand high stresses within electronic packages. The apparent mechanical strength of single crystal Si depends on process induced defects. Mechanical bending tests are the simplest way to obtain the strength of Si dies and wafers and have been used for many years throughout the industry. Some of the bending tests, such as the 3-point-bend (3PB) test, provide a convoluted contribution from both the defects on die surface (caused by backgrinding and mal-handling) and defects on die edges (caused by sawing or dicing). However, the ball-on-ring (BOR) test provides a way to single out the contribution of backside grinding defects to the die strength. This work compares the results of both 3PB and BOR tests on a number of backgrinding and dicing processes. The die strength of the 3PB test is consistently less than that of the BOR test due to the fact that the edge defects are under tension for 3PB tests but not for BOR. It is demonstrated that the BOR test is a good method for backgrinding process optimization. Due to the intrinsic scattering nature of the strength data, a Weibull-based probabilistic mechanics approach is the method of choice to present the data.Keywords
This publication has 13 references indexed in Scilit:
- Fracture toughness improvement of austempered high silicon steel by titanium, vanadium and rare earth elements modificationMaterials Science and Engineering: A, 2007
- Statistical fracture modelling of silicon with varying thicknessActa Materialia, 2006
- Weibull statistics for multiple flaw distributions and its application in silicon fracture prediction2005
- A three-parameter Weibull-like fitting function for flip-chip die strength dataMicroelectronics Reliability, 2004
- The Strength of the Silicon Die in Flip-Chip AssembliesJournal of Electronic Packaging, 2003
- Ball‐on‐Ring Test RevisitedJournal of the American Ceramic Society, 1989
- A Biaxial‐Flexure Test for Evaluating Ceramic StrengthsJournal of the American Ceramic Society, 1983
- Calculated elastic constants for stress problems associated with semiconductor devicesJournal of Applied Physics, 1973
- Young's Modulus, Shear Modulus, and Poisson's Ratio in Silicon and GermaniumJournal of Applied Physics, 1965
- A Statistical Distribution Function of Wide ApplicabilityJournal of Applied Mechanics, 1951