Mechanical Behavior of SiC(f)/SiC Composites and Correlation to in situ Fiber Strength at Room and Elevated Temperatures
Authors:
- 1 March 1996
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 79 (3) , 591-596
Abstract
Mechanical properties of Nicalon‐fiber‐reinforced silicon carbide matrix composites were evaluated, in flexure, at various temperatures ranging from ambient to 1300°C. First matrix cracking stress ranged from 250 to 280 MPa and was relatively insensitive to test temperature. The measured ultimate strength showed a small increase from a room‐temperature value of 370 to 460 MPa at 800°C. Beyond 800°C, however, strength dropped to as low as 280 MPa at 1300°C. This decrease in ultimate strength at elevated temperatures is believed to be partly due to degradation of in situ Nicalon fiber strength. Scanning electron microscopy was employed to evaluate the in situ Nicalon fiber strengths via fracture mirror size measurements. Degradation of Nicalon fiber strength is attributed to thermal damage and to structural changes to the fiber at elevated temperatures. Measured values of ultimate strength of the composites were compared with predictions made on the basis of in situ fiber strength characteristics and an available analytical model.Keywords
This publication has 20 references indexed in Scilit:
- Bend Strength versus Tensile Strength of Fiber‐Reinforced CeramicsJournal of the American Ceramic Society, 1994
- Effect of Fiber Coating on Mechanical Properties of Nicalon Fibers and Nicalon-Fiber/SiC Matrix Composites1994
- Damage Mechanisms and the Mechanical Properties of a Laminated 0/90 Ceramic/Matrix CompositeJournal of the American Ceramic Society, 1992
- Mechanical Properties of Continuous‐Fiber‐Reinforced Carbon Matrix Composites and Relationships to Constituent PropertiesJournal of the American Ceramic Society, 1992
- Effect of Interfaces on the Properties of Fiber‐Reinforced CeramicsJournal of the American Ceramic Society, 1990
- Effect of Interface Mechanical Properties on Pullout in a SiC‐Fiber‐Reinforced Lithium Aluminum Silicate Glass‐CeramicJournal of the American Ceramic Society, 1989
- Strengths of Ceramic Fibers at Elevated TemperaturesJournal of the American Ceramic Society, 1989
- Interface Modification in Nicalon®/SiC Composites1988
- The evaluation of the strength distribution of silicon carbide and alumina fibres by a multi-modal Weibull distributionJournal of Materials Science, 1986
- Thermal Degradation of Nicalon™ SiC Fibers1985