Abstract
The experiments were divided into two groups to establish a drying shrinkage model suitable for modified ceramsite geopolymer concrete (MCGC). In the first experimental group, via comparison with dry ceramsite (untreated), a method for modifying the ceramsite surface with a 6% silicone resin was proposed which could reduce its water absorption, enhance the compressive strength and slump of the corresponding concrete, and decrease the drying shrinkage. The second group systematically explored the influences of control factors on MCGC prepared from modified ceramsite. Different water/binder (w/b) ratios, [Na2O]/b ratios, and metakaolin content (MK/b) ratios were used in the experiment. Compressive strength and drying shrinkage tests were performed for 90 d. High w/b and Na2O/b ratios could enhance drying shrinkage. Moreover, 8% Na2O/b enhanced the compressive strength. Low compressive strength was obtained using 10% Na2O/b. A high MK/b ratio reduced drying shrinkage. However, high w/b and MK/b ratios hindered strength development. Finally, a model predicting drying shrinkage for MCGC with a high prediction accuracy was proposed by considering three control factors. Due to the variety of ceramsite pretreatment methods and the considered factor limitations, the model had potential for additional enhancements.

This publication has 62 references indexed in Scilit: