Inhibition of enamel demineralization and bond-strength properties of bioactive glass containing 4-META/MMA-TBB-based resin adhesive
Authors:
- 22 April 2015
- journal article
- Published by Wiley in European Journal of Oral Sciences
- Vol. 123 (3) , 202-207
Abstract
We investigated the enamel demineralization-prevention ability and shear bond strength (SBS) properties of 4-methacryloxyethyl trimellitic anhydride/methyl methacrylate-tri-n-butyl borane (4-META/MMA-TBB)-based resin containing various amounts (0-50%) of bioactive glass (BG). Disk-shaped specimens were immersed in distilled water and ions released were analysed by inductively coupled plasma atomic-emission spectroscopy. Samples were also immersed in lactic acid solution (pH 4.6) to estimate acid-neutralizing ability. Brackets were bonded to human premolars with BG-containing resins and the bonded teeth were alternately immersed in demineralizing (pH 4.55) and remineralizing (pH 6.8) solutions for 14 d. The enamel hardness was determined by nanoindentation testing at twenty equidistant distances from the external surface. The SBS for each sample was examined. The amounts of ions released [calcium (Ca), sodium (Na), silicon (Si), and boron (B)] and the acid-neutralizing ability increased with increasing BG content. After alternating immersion, the specimens bonded with the BG-containing resin with high BG content were harder than those in the other groups in some locations 1-18.5 μm from the enamel surface. Bioactive glass-containing (10-40%) resin had bond strength equivalent to the control specimen. Thus, the SBS obtained for BG-containing resin (6.5-9.2 MPa) was clinically acceptable, suggesting that this material has the ability to prevent enamel demineralization.Keywords
Funding Information
- Grant-in-Aid for Scientific Research from the Ministry of Education, Culture, Sports, Science and Technology, Japan (No. 24792249)
This publication has 28 references indexed in Scilit:
- Efficacy of a fluoride-releasing orthodontic primer in reducing demineralization around brackets: An in-vivo studyAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2014
- The addition of nano-sized hydroxyapatite to a sports drink to inhibit dental erosion—In vitro study using bovine enamelJournal of Dentistry, 2011
- Enamel and dentine remineralization by nano-hydroxyapatite toothpastesJournal of Dentistry, 2011
- Effect of bracket bonding on nanomechanical properties of enamelAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2010
- Effect of fluoride gels and mouthrinses in combination with saliva substitutes on demineralised bovine enamel in vitroJournal of Dentistry, 2010
- Adhesion of Streptococcus mutans to Different Types of BracketsThe Angle Orthodontist, 2007
- Caries Prevalence Measured with QLF after Treatment with Fixed Orthodontic Appliances: Influencing FactorsCaries Research, 2004
- In vivo inhibition of demineralization around orthodontic bracketsAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2003
- Effects of conventional and high-intensity light-curing on enamel shear bond strength of composite resin and resin-modified glass-ionomerAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2001
- Prevalence of white spot lesions in 19-near-olds: A study on untreated and orthodontically treated persons 5 years after treatmentAmerican Journal of Orthodontics and Dentofacial Orthopedics, 1989