Abstract
A method has been developed for the oxidation of regenerated cellulose (viscose) in the HNO3–H3PO4–NaNO2 system, which makes it possible to obtain oxidized regenerated cellulose with a COOH group content of 18–24% in powder form, which meets USP quality requirements, which allows its use as a biodegradable hemostatic material. The structure of oxidized regenerated celluloses with different contents of COOH groups was confirmed by IR spectroscopy and elemental analysis; the structure of the samples and their thermal stability were studied by X-ray diffraction and thermogravimetric (TG) analyses, respectively. It has been shown that the diffraction patterns of oxidized regenerated celluloses have reflections characteristic of two polymorphs: cellulose II (characteristic of the original regenerated cellulose) and cellulose I. It has been established in the IR spectrum of oxidized regenerated cellulose a band of C=O stretching vibrations of the carboxyl group appears at 1731 cm-1, the intensity of which increases with increasing content of carboxyl groups in oxidized viscose. It has been shown that the degree of crystallinity of oxidized regenerated celluloses obtained in this system decreases proportionally with an increase in the content of carboxyl groups in oxidized viscose, while complete amorphization of viscose is not observed even at the maximum degree of oxidation (24.09% COOH groups). It was founded that at a low catalyst concentration (0.06–0.12%) the viscose oxidation reaction has a pronounced autocatalytic character, and the kinetic curve has a characteristic S-shaped form, while the accumulation of bound nitrogen passed through a maximum and decreases significantly with the reaction time.

This publication has 18 references indexed in Scilit: