Localization and Speciation of Iron Impurities within a Fluid Catalytic Cracking Catalyst
- 5 September 2017
- journal article
- research article
- Published by Wiley in Angewandte Chemie International Edition
- Vol. 56 (45) , 14031-14035
Abstract
Fluid catalytic cracking is a chemical conversion process of industrial scale. This process, utilizing porous catalysts composed of clay and zeolite, converts heavy crude‐oil fractions into transportation fuel and petrochemical feedstocks. Among other factors iron‐rich reactor and feedstream impurities cause these catalyst particles to permanently deactivate. Herein, we report tomographic X‐ray absorption spectroscopy measurements that reveal the presence of dissimilar iron impurities of specific localization within a single deactivated particle. Whereas the iron natural to clay in the composite seems to be unaffected by operation, exterior‐facing and feedstream‐introduced iron was found in two forms. Those being minute quantities of ferrous oxide, located near regions of increased porosity, and impurities rich in Fe3+, preferentially located in the outer dense part of the particle and suggested to contribute to the formation of an isolating amorphous silica alumina envelope.Keywords
Funding Information
- Schweizerischer Nationalfonds zur Förderung der Wissenschaftlichen Forschung (166304, 153556)
This publication has 33 references indexed in Scilit:
- Correlating Metal Poisoning with Zeolite Deactivation in an Individual Catalyst Particle by Chemical and Phase‐Sensitive X‐ray MicroscopyAngewandte Chemie International Edition, 2013
- FCC Catalysts2012
- Three-dimensional imaging of chemical phase transformations at the nanoscale with full-field transmission X-ray microscopyJournal of Synchrotron Radiation, 2011
- Study of the accessibility effect on the irreversible deactivation of FCC catalysts from contaminant feed metalsCatalysis Today, 2007
- A guided tour into subcellular colocalization analysis in light microscopyJournal of Microscopy, 2006
- High-resolution XANES spectra of iron in minerals and glasses: structural information from the pre-edge regionChemical Geology, 2001
- Catalyst attrition in fluidized‐bed systemsAIChE Journal, 1999
- A Multiplet Analysis of Fe K-Edge 1s → 3d Pre-Edge Features of Iron ComplexesJournal of the American Chemical Society, 1997
- Monitoring Fluid Cracking Catalyst Deactivation Profile by Equilibrium Catalyst Separation1991
- Isomorphous Substitution of Iron in the Faujasite Lattice1989