Effect of organoclay reinforcement on the curing characteristics and technological properties of styrene–butadiene rubber
- 19 April 2014
- journal article
- research article
- Published by Wiley in Polymer Composites
- Vol. 36 (7) , 1293-1302
Abstract
Rubber nanocomposites based on styrene–butadiene rubber (SBR) and organophilic layered silicate were prepared. Clay structures based on dodecyl benzene sulfonic acid (DBSA), nonyl phenol ethoxylate (NPE), and DBSA/NPE (50/50%) were prepared and characterized. The results indicate the intercalation of the used surfactants within the clay layers. Varying amount of organoclay, 2, 4, 6, 8, and 10 (phr), was added to the SBR matrix. X‐ray diffraction revealed exfoliated structure for the modified clay–SBR composites. No new component in the rubber was found by fourier transform infrared measurements (FTIR). Scanning electron microscopy showed a uniform distribution of the modified clay with mixed DBSA/NPE (6 phr) in the matrix. The rheometric characteristics and physicomechanical properties of the SBR compounds were analyzed. The effect of DBSA/NPE clay loading on aging resistance of SBR nanocomposites at 90 ± 1°C for 4 and 7 days was also investigated. Rubber nanocomposites displayed an increase in the minimum and maximum torques, acceleration of the vulcanization process, and improved mechanical properties, with organoclay content up to 6 phr. This effect was more noticeable in the presence of the treated clay with DBSA/NPE. Also incorporation of DBSA/NPE‐clay (6 phr) resulted in significant improvement of the degradation profile of the nanocomposites at 90 ± 1°C for 4 days. POLYM. COMPOS., 36:1293–1302, 2015. © 2014 Society of Plastics EngineersKeywords
This publication has 41 references indexed in Scilit:
- Exfoliated/intercalated silicate/hot styrene butadiene rubber nanocomposites: Structure–properties relationshipJournal of Applied Polymer Science, 2012
- Microstructure, morphology, and mechanical properties of styrene‐butadiene rubber/organoclay nanocompositesPolymer Engineering & Science, 2011
- SBR/organoclay nanocomposites for the application on tire tread compoundsMacromolecular Research, 2009
- Preparation and properties of organo-montmorillonite/cis-1,4-polybutadiene rubber nanocomposites by solution intercalationApplied Clay Science, 2009
- Styrene-butadiene rubber/halloysite nanotubes nanocomposites modified by sorbic acidApplied Surface Science, 2009
- Preparation and Properties of Nanostructured Rubber Composites with MontmorilloniteMacromolecular Symposia, 2007
- Preparation and properties of nitrile rubber/montmorillonite nanocomposites via latex blendingJournal of Materials Science, 2006
- Structure and properties of polybutadiene/montmorillonite nanocomposites prepared by in situ polymerizationJournal of Applied Polymer Science, 2006
- On the potential of organoclay with respect to conventional fillers (carbon black, silica) for epoxidized natural rubber compatibilized natural rubber vulcanizatesJournal of Applied Polymer Science, 2004
- Rubber Nanocomposites: Morphology and Mechanical Properties of BR and SBR Vulcanizates Reinforced by Organophilic Layered SilicatesRubber Chemistry and Technology, 2001