Intermediate-temperature oxidation behavior of Ti2AlC in air
Authors:
- 1 November 2002
- journal article
- Published by Springer Nature in Journal of Materials Research
- Vol. 17 (11) , 2974-2981
Abstract
The isothermal oxidation behavior of Ti2AlC at intermediate temperatures of 500, 600, 700, 800, and 900 °C in flowing air was investigated by means of thermogravimetric analysis, x-ray diffraction (XRD), Raman spectroscopy, and scanning electron microscopy (SEM)/energy dispersive spectroscopy. An anomalous oxidation with higher kinetics at lower temperatures of 500 and 600 °C was observed although Ti2AlC exhibited good oxidation resistance at higher temperatures. As revealed by SEM scale morphology observation, oxidation-induced cracks present at temperatures of 500 and 600 °C resulted in poor protectivity of scales and accounted for the anomalous oxidation. The weight gain data for the remaining temperatures were analyzed with an instantaneous parabolic rate constant method by assuming a parabolic rate law. The variations of instantaneous parabolic rate constant with time reflected the complexity of the oxidation behavior of Ti2AlC at intermediate temperatures. These variations were discussed from the viewpoint of phase transformation of oxidation products on the basis of XRD, Raman spectroscopy, and SEM scale morphology observation. As indicated by XRD and Raman spectra, the scale formed on Ti2AlC at higher temperature was stable α–Al2O3 and rutile TiO2, while transition aluminas of γ–Al2O3, δ–Al2O3, θ–Al2O3, and TiO2 (anatase) were detected at lower temperatures. The whisker morphology of θ–Al2O3 at 800 °C and ridged morphology of α–Al2O3 at 800 and 900 °C were confirmed by SEM.Keywords
This publication has 22 references indexed in Scilit:
- Solid-Liquid Reaction Synthesis and Simultaneous Densification of Polycrystalline Ti2AlCZeitschrift für Metallkunde, 2002
- Deformation of polycrystalline Ti2AlC under compressionMaterials Research Innovations, 2001
- Processing and characterization of Ti2AlC, Ti2AlN, and Ti2AlC0.5N0.5Metallurgical and Materials Transactions A, 2000
- Oxidation behavior of titanium aluminides of high niobium contentIntermetallics, 2000
- Electronic structure and bonding properties of layered machinableandceramicsPhysical Review B, 2000
- Layered machinable ceramics for high temperature applicationsScripta Materialia, 1997
- High-temperature oxidation of Ti3Al-based titanium aluminides in oxygenMetallurgical and Materials Transactions A, 1996
- Oxidation of β‐FeAl and Fe‐Al alloysMaterials and Corrosion, 1996
- Summary of constitutional data on the Aluminum-Carbon-Titanium systemJournal of Phase Equilibria and Diffusion, 1994
- Solid-state synthesis and characterization of the ternary phase Ti3SiC2Journal of Materials Science, 1994