On the upper limit of content in tetrahedral amorphous carbon film
Authors:
- 1 January 1999
- journal article
- Published by IOP Publishing in Journal of Physics: Condensed Matter
- Vol. 11 (1) , 185-189
Abstract
The morphological properties of the tetrahedral amorphous carbon (ta-C) films deposited by the filtered cathodic vacuum arc (FCVA) technique have been studied over the carbon ion energy range 15 to 200 eV. All the films studied are very smooth with a roughness below 0.6 nm. The minimum roughness ( nm) occurs at the highest content. The lateral feature size increases with ion energy. There appear to be two different growth mechanisms before and after the peak content. The morphological result suggests an upper limit content of about 89% in the ta-C films deposited by FCVA technique.Keywords
This publication has 14 references indexed in Scilit:
- The structure of tetrahedral amorphous carbon thin filmsThin Solid Films, 1996
- Hydrogen-free amorphous carbon films: correlation between growth conditions and propertiesDiamond and Related Materials, 1996
- Hardness, elastic modulus, and structure of very hard carbon films produced by cathodic-arc deposition with substrate pulse biasingApplied Physics Letters, 1996
- Properties of amorphous diamond films prepared by a filtered cathodic arcJournal of Applied Physics, 1995
- The effect of ion energy on the diamond-like/graphitic (sp3/sp2) nature of carbon films deposited by ion beamsDiamond and Related Materials, 1994
- Fabrication of amorphous diamond filmsThin Solid Films, 1993
- Properties of filtered-ion-beam-deposited diamondlike carbon as a function of ion energyPhysical Review B, 1993
- Deposition of TiN, TiC, and TiO2 films by filtered arc evaporationSurface and Coatings Technology, 1991
- Compressive-stress-induced formation of thin-film tetrahedral amorphous carbonPhysical Review Letters, 1991
- Structure and hardness of diamond-like carbon films prepared by arc evaporationJournal of Materials Science Letters, 1988