CaCl2-induced interfacial deposition for the preparation of high-strength and flame-retardant plywood using geopolymer-based adhesive
Authors:
- Dawei PanDPDawei Pan
- Na ZhangNZNa Zhang
- Jingyu LiJLJingyu Li
- Hanzhou YeHYHanzhou Ye
- Zhiming YuZYZhiming Yu
- Yang ZhangYZYang Zhang
- 1 December 2021
- journal article
- research article
- Published by Elsevier in Ceramics International
- Vol. 47 (23) , 33678-33686
Abstract
No abstract availableKeywords
Funding Information
- National Natural Science Foundation of China (31800485)
This publication has 61 references indexed in Scilit:
- Adhesion at interface of geopolymer and cement mortar under compression: An experimental studyConstruction and Building Materials, 2012
- FTIR-ATR-based prediction and modelling of lignin and energy contents reveals independent intra-specific variation of these traits in bioenergy poplarsPlant Methods, 2011
- Functionalization by Reductive Alkylation and Mapping of a Subbituminous Coal by Energy Dispersive X-ray SpectroscopyEnergy & Fuels, 2011
- Ion exchange in the charge-balancing sites of aluminosilicate inorganic polymersJournal of Materials Chemistry, 2010
- Fly ash based geopolymer thin coatings on metal substrates and its thermal evaluationJournal of Hazardous Materials, 2010
- Composition design and microstructural characterization of calcined kaolin-based geopolymer cementApplied Clay Science, 2010
- Adhesion characterization of tungsten mine waste geopolymeric binder. Influence of OPC concrete substrate surface treatmentConstruction and Building Materials, 2008
- The coexistence of geopolymeric gel and calcium silicate hydrate at the early stage of alkaline activationCement and Concrete Research, 2005
- The reaction between rice husk ash and Ca(OH)2 solution and the nature of its productCement and Concrete Research, 1999
- Early microstructure development of activated lime-fly ash pastesCement and Concrete Research, 1996