Diffusion bonding of tantalum and stainless steel

Authors:

Abstract
This paper describes an investigation of diffusion bonding of commercially pure tantalum and austenitic stainless steel SUS304 in a vacuum of 8 mPa at temperatures ranging between 600–1200°C. Direct bonding of tantalum and stainless steel results in extremely low joint strength and formation of intermetallic compounds, such as e.g. FeTa, Fe7Ta3, NiTa2, NiTa, Ni2Ta, Ni3Ta, Ni8Ta, and Cr2Ta in the joint bond zone. To examine the effects of stainless steel alloying elements such as e.g. Cr, C, Fe and Ni on the joint strength, diffusion bonding was performed between tantalum and pure chromium, tantalum and carbon steel (0.42 mass%C), tantalum and pure iron, and tantalum and pure nickel. The effects of Fe, Ni and Cu foil inserts on the strength of tantalum and stainless steel joints were also studied. The results obtained may be summarised as follows: