Temperature and strain rate effect on tensile properties of 9Cr–1·8W–0·5Mo–VNb steel
Authors:
- T. SakthivelTST. Sakthivel
- K. LahaKLK. Laha
- P. ParameswaranPPP. Parameswaran
- S. Paneer SelviSSS. Paneer Selvi
- M. D. MathewMMM. D. Mathew
- 29 October 2014
- journal article
- Published by Taylor & Francis in Materials at High Temperatures
- Vol. 32 (4) , 377-383
Abstract
No abstract availableKeywords
This publication has 28 references indexed in Scilit:
- Microstructures and mechanical properties of creep resistant steel for application at elevated temperaturesMaterials & Design (1980-2015), 2013
- Microstructure Evolution in an Advanced 9 pct Cr Martensitic Steel during Creep at 923 K (650 °C)Metallurgical and Materials Transactions A, 2012
- Microstructure Evolution and Pinning of Boundaries by Precipitates in a 9 pct Cr Heat Resistant Steel During CreepMetallurgical and Materials Transactions A, 2011
- Modelling creep behaviour and failure of 9Cr–0.5Mo–1.8W–VNb steelInternational Journal of Pressure Vessels and Piping, 2009
- Phase evolution in P92 and E911 weld metals during ageingMaterials Science and Engineering: A, 2008
- Creep behavior and stability of MX precipitates at high temperature in 9Cr–0.5Mo–1.8W–VNb steelMaterials Science and Engineering: A, 2001
- Creep rates and strengthening mechanisms in tungsten-strengthened 9Cr steelsMaterials Science and Engineering: A, 2001
- Advances in Physical Metallurgy and Processing of Steels. Strengthening Mechanisms of Creep Resistant Tempered Martensitic Steel.ISIJ International, 2001
- Influence of heat treatments on microstructural parameters and mechanical properties of P92 steelMaterials Science and Technology, 2000
- Microstructural stability and creep rupture strength of the martensitic steel P92 for advanced power plantActa Materialia, 1997